A new method is described in which raw materials prepared by mixing kaolin and concentrated acid are heated in a furnace at temperatures between 100 and 700degreesC. Experiments with HCl, HNO3, H3PO4, and H2SO4 showed that only, H2SO4 gave high reaction yields, which grew steadily as reaction temperature was raised. Reaction products were mostly Al-2(SO4)(3). Leached kaolin samples showed BET specific surface areas of over 100 m(2) g(-1). Furthermore, reaction between kaolin and H2SO4 required no previous calcination of kaolin.
引用
收藏
页码:203 / 206
页数:4
相关论文
共 29 条
[11]  
GARCIACLAVEL ME, 1979, Patent No. 482881
[12]  
GARCIACLAVEL ME, 1985, Patent No. 545690
[13]   CHLORINATION OF ALUMINA IN KAOLINITIC CLAY [J].
GROB, B ;
RICHARZ, W .
METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1984, 15 (03) :529-533
[14]  
GROB B, 1983, THESIS ETH ZURICH SW
[15]  
Hinckley DN., 1962, CLAYS CLAY MINER, V11, P229, DOI [10.1346/ccmn.1962.0110122, DOI 10.1346/CCMN.1962.0110122]
[16]  
Hulbert S.F., 1970, CLAY MINER, V8, P337, DOI DOI 10.1180/CLAYMIN.1970.008.3.11
[17]   SUBSTITUTION BY IRON IN KAOLINITE [J].
MALDEN, PJ ;
MEADS, RE .
NATURE, 1967, 215 (5103) :844-&
[18]  
MARTIN ES, 1978, Patent No. 4086320
[19]  
MARTIN ES, 1978, Patent No. 4096234
[20]  
MARTIN ES, 1984, LIGHT MET, P619