Effect of 4 wt.% Cr on microstructure, corrosion resistance and tribological properties of Fe3Al-20 wt.%Al2O3 composites

被引:18
|
作者
Bai, Yaping [1 ]
Xing, Jiandong [1 ]
Ma, Shengqiang [1 ]
Huang, Qian [1 ]
He, Yuanyuan [1 ]
Liu, Zhen [1 ]
Gao, Yimin [1 ]
机构
[1] Xi An Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Mech Behav Mat, Xian 710049, Shaanxi, Peoples R China
关键词
Microstructure; Corrosion resistance; Tribological properties; Fe3Al-20 wt.%Al2O3 composites; Cr element; SLIDING WEAR BEHAVIOR; MECHANICAL-PROPERTIES; CHROMIUM; ALLOYS; EMBRITTLEMENT; FRICTION; FE-28AL; MATRIX;
D O I
10.1016/j.matchar.2013.01.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fe3Al-20 wt.%Al2O3 ultrafine grained composites with 4 wt.% Cr were prepared by mechanical alloying inducing self propagating high temperature synthesis with subsequent plasma activated sintering. Microstructures of the composites were studied by X-ray diffraction, scanning electron microscopy, energy dispersive spectrum and transmission electron microscope. Then the relative density, room temperature hardness, static corrosion resistance and dry sliding wear behavior at a temperature range of 25 degrees C-800 degrees C of the sintered samples were tested and analyzed. The results showed that the composites had high hardness and a good microstructure with fine grain size, high relative density. The composites with 4 wt.% Cr amount also exhibited excellent comprehensive tribological properties at medium-high temperatures especially at a temperature above 500 degrees C, although the wear resistance did not be improved at 25 degrees C-500 degrees C. 4 wt.% Cr element addition improved the corrosion resistance of the composites significantly with the corrosion loss decreasing by 19.48%. (c) 2013 Elsevier Inc. All rights reserved.
引用
收藏
页码:69 / 78
页数:10
相关论文
共 50 条
  • [1] Study on preparation and mechanical properties of Fe3Al-20 wt.%Al2O3 composites
    Bai, Yaping
    Xing, Jiandong
    Wu, Haoliang
    Liu, Zhen
    Gao, Yimin
    Ma, Shengqiang
    MATERIALS & DESIGN, 2012, 39 : 211 - 219
  • [2] Tribological behavior of in-situ (Cr, Mo)/Fe3Al-20 wt.%Al2O3 composites at elevated temperatures
    Bai, Yaping
    Xing, Jiandong
    He, Yuanyuan
    Liu, Zhen
    Huang, Qian
    Ma, Shengqiang
    Gao, Yimin
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2014, 228 (08) : 904 - 912
  • [3] Tribological properties of in situ Fe3Al-20 wt% Al2O3 composites
    Bai, Yaping
    Xing, Jiandong
    Liu, Zhen
    Wu, Haoliang
    Ma, Shengqiang
    Huang, Qian
    Gao, Yimin
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2013, 227 (J1) : 67 - 78
  • [4] Influence of 4 wt.% Cr addition on the corrosion-wear synergistic effect for Al2O3/Fe(Al) composites
    Bai, Yaping
    Xing, Jiandong
    Guo, Yongchun
    Li, Jianping
    Huang, Qian
    Gao, Yimin
    CORROSION REVIEWS, 2016, 34 (04) : 231 - 240
  • [5] Effect of Cr on Microstructure, Mechanical Properties, and Wear Behavior of In Situ 20 wt.%Al2O3/Fe-25Al Composites
    Bai, Yaping
    Xing, Jiandong
    Guo, Yongchun
    Li, Jianping
    He, Yuanyuan
    Ma, Shengqiang
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (02) : 936 - 945
  • [6] Effect of Cr on Microstructure, Mechanical Properties, and Wear Behavior of In Situ 20 wt.%Al2O3/Fe-25Al Composites
    Yaping Bai
    Jiandong Xing
    Yongchun Guo
    Jianping Li
    Yuanyuan He
    Shengqiang Ma
    Journal of Materials Engineering and Performance, 2015, 24 : 936 - 945
  • [7] Effect of MoS2 on the tribological properties of in situ Fe3Al-20wt% Al2O3-4wt% Cr composites
    Bai, Yaping
    Xing, Jiandong
    Ma, Shengqiang
    He, Yuanyuan
    Liu, Zhen
    Huang, Qian
    Gao, Yimin
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2013, 227 (09) : 1018 - 1029
  • [8] Relationship between microstructure, hardness and corrosion resistance in 20 wt.%Cr, 27 wt.%Cr and 36 wt.%Cr high chromium cast irons
    Wiengmoon, A.
    Pearce, J. T. H.
    Chairuangsri, T.
    MATERIALS CHEMISTRY AND PHYSICS, 2011, 125 (03) : 739 - 748
  • [9] Microwave sintering and mechanical properties of Y-TZP/20 wt.% Al2O3 composites
    Travitzky, NA
    Goldstein, A
    Avsian, O
    Singurindi, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 286 (02): : 225 - 229
  • [10] Corrosion behaviors of Cr2AlC/α-Al2O3 composites in 3.5 wt. % NaCl aqueous solution
    Zhang, Zerong
    Qian, Yuhai
    Xu, Jingjun
    Zuo, Jun
    Li, Meishuan
    CERAMICS INTERNATIONAL, 2020, 46 (08) : 11846 - 11853