Influence of heat treated microstructures on the dynamic deformation characteristics of Ti-6Al-4V alloy

被引:4
作者
Seo, Yongseok [1 ]
Woo, Sung-Choong [2 ]
Kim, Tae-Won [3 ]
Lee, Young-Shin [1 ]
机构
[1] Chungnam Natl Univ, Dept Mech Design Engn, Taejon 305764, South Korea
[2] Hanyang Univ, Survivabil Technol Def Res Ctr, Seoul 133791, South Korea
[3] Hanyang Univ, Sch Mech Engn, Seoul 133791, South Korea
关键词
Ti-6Al-4V alloy; Microstructure; Dynamic deformation; Shear crack; Compressive SHPB test; BALLISTIC IMPACT BEHAVIOR; MECHANICAL-PROPERTIES; TEMPERATURE; FRACTURE;
D O I
10.1007/s12206-015-1122-x
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
We investigated the influence of heat treated microstructures, namely, equiaxed, bimodal and lamella types of Ti-6Al-4V alloy on the dynamic deformation characteristics. Four different heat treatment conditions were employed for the development of the microstructures. Static tensile and compressive deformation tests were preliminarily performed with hydraulic test equipment. Dynamic deformation tests at a high level of strain rate, 2700 s(-1) similar to 6400 s(-1), together with high velocity impact tests were, respectively, conducted on the specimens through a compressive Split Hopkinson pressure bar (SHPB) and a high pressure gas gun system. The dependence of flow stress on the strain rate associated with the corresponding microstructure was examined. The microstructural factors on the dynamic fracture characteristics were analyzed by scanning electron microscopy. The static compressive tests showed that the flow stress was greatest in the lamella microstructure and decreased in the order of lamella, bimodal and equiaxed microstructures, whereas the ductility was largest in the bimodal microstructure and smallest in the lamellar microstructure. In dynamic compressive tests, a similar dependency of the flow stress on microstructures was observed: highest in the lamellar microstructure and lowest in the equiaxed microstructure. The ductility, such as strain at maximum stress or at failure, was highest in the equiaxed microstructure and lowest in the lamellar structure. In addition, the ductility for individual microstructure decreased as the strain rate increased. Every microstructure exhibited ductile fracture surfaces, and it seems that a large shear crack on the lateral surface in the specimen was the main factor inducing the final failure. The result of high velocity impact test exhibited that the resistance to fracture of equiaxed microstructure with superior dynamic toughness was much higher than that of lamella microstructure with inferior dynamic toughness. The results obtained help provide a fundamental idea and guide to improve the dynamic mechanical properties of Ti-6Al-4V alloy through the microstructure control.
引用
收藏
页码:5223 / 5232
页数:10
相关论文
共 23 条
  • [1] A study of the mechanism of α to β phase transformation by tracking texture evolution with temperature in Ti-6Al-4V using neutron diffraction
    Bhattacharyya, D
    Viswanathan, GB
    Vogel, SC
    Williams, DJ
    Venkatesh, V
    Fraser, HL
    [J]. SCRIPTA MATERIALIA, 2006, 54 (02) : 231 - 236
  • [2] EYLON D, 1976, METALL TRANS A, V7, P1817, DOI 10.1007/BF02654976
  • [3] MECHANISM OF VOID FORMATION, VOID GROWTH, AND TENSILE FRACTURE IN AN ALLOY CONSISTING OF 2 DUCTILE PHASES
    GREENFIE.MA
    MARGOLIN, H
    [J]. METALLURGICAL TRANSACTIONS, 1972, 3 (10): : 2649 - &
  • [4] INFLUENCE OF TEST TEMPERATURE AND MICROSTRUCTURE ON THE TENSILE PROPERTIES OF TITANIUM-ALLOYS
    GYSLER, A
    LUTJERING, G
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (08): : 1435 - 1443
  • [5] An experimental study on the ballistic impact behavior of some metallic armour materials against 7.62 mm deformable projectile
    Jena, Pradipta Kumar
    Mishra, Bidyapati
    Kumar, K. Siva
    Bhat, T. Balakrishna
    [J]. MATERIALS & DESIGN, 2010, 31 (07): : 3308 - 3316
  • [6] Through thickness dynamic impact response in textured Ti-6Al-4V plates
    Kad, BK
    Schoenfeld, SE
    Burkins, MS
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 322 (1-2): : 241 - 251
  • [7] EXPERIMENTAL STUDIES IN PLASTIC WAVE PROPAGATION
    KOLSKY, H
    DOUCH, LS
    [J]. JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1962, 10 (03) : 195 - 223
  • [8] Quasi-static and dynamic deformation behavior of Ti-6A1-4V alloy containing fine α2-Ti3Al precipitates
    Lee, DG
    Lee, S
    Lee, CS
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 366 (01): : 25 - 37
  • [9] Plastic deformation and fracture behaviour of Ti-6Al-4V alloy loaded with high strain rate under various temperatures
    Lee, WS
    Lin, CF
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 241 (1-2): : 48 - 59
  • [10] Micro-damage of Ti-6Al-4V alloy under hypervelocity projectile impact
    Li, HT
    Zhang, YM
    Yang, DZ
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 292 (01): : 130 - 132