Failure analysis of glazed LAS glass-ceramic containing cerium oxide

被引:11
作者
Barbi, Silvia [1 ]
Miselli, Paola [1 ]
Siligardi, Cristina [1 ]
机构
[1] Univ Modena & Reggio Emilia, Dept Engn Enzo Ferrari, I-41125 Modena, Italy
关键词
LAS; Glass-ceramic; Flexural strength; Cerium oxide; Glaze; THERMAL-EXPANSION; PHASE; STRENGTH;
D O I
10.1016/j.ceramint.2016.10.117
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study a deep investigation of the correlation between microstructure and mechanical properties was performed on glass-ceramic materials containing cerium oxide. The glass-ceramic materials investigated were lithium-aluminum silicate based (LAS), obtained through different thermal cycles from the same parent glass. The mechanical properties were tested on the glass-ceramics with and without the application of a glaze. All the glass-ceramics were characterized by means of scanning electron microscopy (SEM), also in field emission guns geometry (FEG), energy-dispersive spectrometry (EDS), X-Ray diffraction (XRD), and 3-points mechanical flexural strength resistance test. This study has revealed that the microstructure of the glass-ceramic is mainly affected by the heating treatments holding times. The application of a glass coating leads to the formation of cerium oxide crystals at the glaze/glass-ceramic interface. This phenomenon is one of the main principal causes of the mechanical properties failure when a glaze is applied.
引用
收藏
页码:1472 / 1478
页数:7
相关论文
共 21 条
[1]   Effect of sandblasting, grinding, polishing and glazing on the flexural strength of two pressable all-ceramic dental materials [J].
Albakry, M ;
Guazzato, M ;
Swain, MV .
JOURNAL OF DENTISTRY, 2004, 32 (02) :91-99
[2]  
Barbi Silvia, 2016, Key Engineering Materials, V702, P28, DOI 10.4028/www.scientific.net/KEM.702.28
[3]   DESIGN AND PROPERTIES OF GLASS-CERAMICS [J].
BEALL, GH .
ANNUAL REVIEW OF MATERIALS SCIENCE, 1992, 22 :91-119
[4]   The development and testing of glaze materials for application to the fit surface of dental ceramic restorations [J].
Cattell, Michael J. ;
Chadwick, Thomas C. ;
Knowles, Jonathan C. ;
Clarke, Richard L. .
DENTAL MATERIALS, 2009, 25 (04) :431-441
[5]   Phase and microstructure formation and their influence on the strength of two types of glass-ceramics [J].
Dittmer, M. ;
Ritzberger, C. ;
Schweiger, M. ;
Rheinberger, V. ;
Woerle, M. ;
Hoeland, W. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2014, 384 :55-60
[6]  
ElMeliegy E, 2012, GLASSES AND GLASS CERAMICS FOR MEDICAL APPLICATIONS, P1, DOI 10.1007/978-1-4614-1228-1
[7]  
Ferrari G., 1987, INTERCERAM, V36, P27
[8]   Accuracy in quantitative phase analysis of mixtures with large amorphous contents. The case of stoneware ceramics and bricks [J].
Gualtieri, Alessandro F. ;
Riva, Vincenzo ;
Bresciani, Andrea ;
Maretti, Stefano ;
Tamburini, Marco ;
Viani, Alberto .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2014, 47 :835-846
[9]  
Holand W., 2002, Glass-ceramic technology
[10]   Phase transformations of Li2O-Al2O3-SiO2 glasses with CeO2 addition [J].
Hu, AM ;
Liang, KM ;
Zhou, F ;
Wang, GL ;
Peng, F .
CERAMICS INTERNATIONAL, 2005, 31 (01) :11-14