Influence of surface pretreatments on the corrosion protection of sol-gel coated AA2024-T3 aluminium alloy

被引:21
作者
Feng, Z. [1 ]
Liu, Y. [1 ]
Hashimoto, T. [1 ]
Thompson, G. E. [1 ]
Zhou, X. [1 ]
Skeldon, P. [1 ]
机构
[1] Univ Manchester, Sch Mat, Ctr Corros & Protect, Manchester M13 9PL, Lancs, England
基金
英国工程与自然科学研究理事会;
关键词
sol-gel coatings; AA2024-T3 aluminium alloy; alkaline etching; acid cleaning; 2ND PHASE; COATINGS;
D O I
10.1002/sia.5216
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present study, the effects of surface pretreatments of AA2024 aluminium alloy on the corrosion protection of the alloy using a sol-gel coating were investigated. It was revealed that the second phase particles that remain after etching and desmutting have a significant impact on the subsequent sol-gel coating which, in turn, influences the overall corrosion protection afforded to the substrate by the sol-gel coating. The removal of second phase particles in the surface region can be achieved by an alternative surface pretreatment using nitric acid. A significant improvement of corrosion protection of sol-gel coated AA2024 aluminium alloy was observed when the surface of the alloy was pretreated with nitric acid. Copyright (c) 2013 John Wiley & Sons, Ltd.
引用
收藏
页码:1452 / 1456
页数:5
相关论文
共 16 条
[1]   Self-assembled NAnophase Particle (SNAP) surface treatments for corrosion protection of AA2024-T3 [J].
Donley, MS ;
Balbyshev, VN ;
Voevodin, NN .
PROGRESS IN ORGANIC COATINGS, 2005, 52 (01) :34-38
[2]   The self-assembled nanophase particle (SNAP) process: a nanoscience approach to coatings [J].
Donley, MS ;
Mantz, RA ;
Khramov, AN ;
Balbyshev, VN ;
Kasten, LS ;
Gaspar, DJ .
PROGRESS IN ORGANIC COATINGS, 2003, 47 (3-4) :401-415
[3]  
Du YJ, 2001, PROG ORG COAT, V41, P226
[4]   Sol-gel coatings for corrosion protection of 1050 aluminium alloy [J].
Feng, Z. ;
Liu, Y. ;
Thompson, G. E. ;
Skeldon, P. .
ELECTROCHIMICA ACTA, 2010, 55 (10) :3518-3527
[5]   Crack-free sol-gel coatings for protection of AA1050 aluminium alloy [J].
Feng, Z. ;
Liu, Y. ;
Thompson, G. E. ;
Skeldon, P. .
SURFACE AND INTERFACE ANALYSIS, 2010, 42 (04) :306-310
[6]   A morphological study of filiform corrosive attack on cerated AA2024-T351 aluminium alloy [J].
Hughes, AE ;
Mol, JMC ;
Hinton, BRW ;
van der Zwaag, S .
CORROSION SCIENCE, 2005, 47 (01) :107-124
[7]   Surface morphological changes of aluminium alloys in alkaline solution: effect of second phase material [J].
Koroleva, EV ;
Thompson, GE ;
Hollrigl, G ;
Bloeck, M .
CORROSION SCIENCE, 1999, 41 (08) :1475-1495
[8]   Anodic behaviour of a model second phase: Al-20at.%Mg-20at.%Cu [J].
Liu, Y. ;
Arenas, M. A. ;
Skeldon, P. ;
Thompson, G. E. ;
Bailey, P. ;
Noakes, T. C. Q. ;
Habazaki, H. ;
Shimizu, K. .
CORROSION SCIENCE, 2006, 48 (05) :1225-1248
[9]   Comparison of the behaviours of chromate and sol-gel coatings on aluminium [J].
Liu, Y. ;
Feng, Z. ;
Walton, J. ;
Thompson, G. E. ;
Skeldon, P. ;
Zhou, X. .
SURFACE AND INTERFACE ANALYSIS, 2013, 45 (10) :1446-1451
[10]   Pre-treatment of AA6060 aluminium alloy for adhesive bonding [J].
Lunder, O ;
Olsen, B ;
Nisancioglu, K .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2002, 22 (02) :143-150