Mode-I intralaminar fracture toughness of silica particles-filled glass woven fabric-reinforced vinyl ester composites

被引:4
作者
Prasad, M. S. Sham [1 ]
Venkatesha, C. S. [2 ]
Jayaraju, T. [1 ]
Janardhan, D. [3 ]
机构
[1] Natl Inst Engn, Dept Mech Engn, Mysore 570008, Karnataka, India
[2] U BDT Coll Engn, Dept Mech Engn, Davangere 577004, India
[3] MES Coll Sci Arts & Commerce, Dept Stat, Bangalore, Karnataka, India
关键词
Polymer matrix composites; Silica particles; Intralaminar fracture toughness; INTERLAMINAR FRACTURE; EPOXY COMPOSITES; FAILURE; BEHAVIOR; TENSILE; RESINS;
D O I
10.1002/pc.22208
中图分类号
TB33 [复合材料];
学科分类号
摘要
Glass woven fabric reinforced vinyl ester (GV) composites filled with different weight proportions of silica particles were fabricated by hand lay up technique followed by oven curing. The plane strain Mode-I Intralaminar fracture toughness, KIC of the silica filled GV composites has been studied and the experimental results were compared with those of unfilled GV composites. The findings of the experiments showed that the fracture toughness has improved by the addition of silica particles up to 6 weight % with marginal increase of tensile properties. The silica filled and unfilled GV composites showed brittle fracture, with maximum toughness for 6 weight % silica particles. The morphology of fracture surfaces was examined by using SEM. Pulled and fractured fibers are observed on the fracture surface of GV composites evidencing fiber bridging but not in the silica filled GV composites. POLYM. COMPOS., 2012. (c) 2012 Society of Plastics Engineers
引用
收藏
页码:789 / 795
页数:7
相关论文
共 24 条
[1]  
[Anonymous], 1999, Annual Book of ASTM Standards
[2]  
Bascom W.D., 1980, ADHESION, V6
[3]   Delamination fracture of multidirectional carbon-fiber/epoxy composites under Mode I, Mode II and Mixed-Mode I/II loading [J].
Choi, NS ;
Kinloch, AJ ;
Williams, JG .
JOURNAL OF COMPOSITE MATERIALS, 1999, 33 (01) :73-100
[4]   MEASUREMENT OF GIC AND GIIC IN CARBON EPOXY COMPOSITES [J].
DAVIES, P ;
MOULIN, C ;
KAUSCH, HH ;
FISCHER, M .
COMPOSITES SCIENCE AND TECHNOLOGY, 1990, 39 (03) :193-205
[5]   An experimental study of scale effects in marine composites [J].
Davies, P ;
Petton, D .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (03) :267-275
[6]   ROUND-ROBIN INTERLAMINAR FRACTURE TESTING OF CARBON-FIBER-REINFORCED EPOXY AND PEEK COMPOSITES [J].
DAVIES, P ;
KAUSCH, HH ;
WILLIAMS, JG ;
KINLOCH, AJ ;
CHARALAMBIDES, MN ;
PAVAN, A ;
MOORE, DR ;
PREDIGER, R ;
ROBINSON, I ;
BURGOYNE, N ;
FRIEDRICH, K ;
WITTICH, H ;
REBELO, CA ;
MARQUES, AT ;
RAMSTEINER, F ;
MELVE, B ;
FISCHER, M ;
ROUX, N ;
MARTIN, D ;
CZARNOCKI, P ;
NEVILLE, D ;
VERPOEST, I ;
GOFFAUX, B ;
LEE, R ;
WALLS, K ;
TRIGWELL, N ;
PARTRIDGE, IK ;
JAUSSAUD, J ;
ANDERSEN, S ;
GIRAUD, Y ;
HALE, G ;
MCGRATH, G .
COMPOSITES SCIENCE AND TECHNOLOGY, 1992, 43 (02) :129-136
[7]  
Funk JG, 1989, 2950 NASA
[8]   FAILURE MECHANISMS IN TOUGHENED EPOXY-RESINS - A REVIEW [J].
GARG, AC ;
MAI, YW .
COMPOSITES SCIENCE AND TECHNOLOGY, 1988, 31 (03) :179-223
[9]   INTRALAMINAR AND INTERLAMINAR FRACTURE IN GRAPHITE EPOXY LAMINATES [J].
GARG, AC .
ENGINEERING FRACTURE MECHANICS, 1986, 23 (04) :719-733
[10]  
Greene E., 1990, 360 SSC, P360