Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature

被引:44
|
作者
Choi, Jeong-Won [1 ]
Aoki, Yasuhiro [1 ]
Ushioda, Kohsaku [1 ]
Fujii, Hidetoshi [1 ]
机构
[1] Osaka Univ, Joining & Welding Res Inst, Osaka, Ibaraki 5670047, Japan
基金
日本学术振兴会;
关键词
Interfacial temperature; Microstructure; Mechanical properties; Linear friction welding (LFW); Ti alloys; MICROSTRUCTURE; BEHAVIOR;
D O I
10.1016/j.scriptamat.2020.09.013
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The interfacial temperature, microstructure and hardness distribution of the linear friction welded Ti-6Al-4V joints obtained at different applied pressures were investigated. The sound Ti-6Al-4V alloy joints were successfully fabricated below the beta-phase transformation temperature. The increased pressure considerably decreased the welding temperature. The dynamically recrystallized ultra-fined alpha equiaxed grains of 0.2 mu m were formed in the weld center of the joint by applying pressure of 550 MPa. Moreover, the hardness of the weld center was higher than that of the base material without the softened region in thermo-mechanical affected zone, which suggests the improved mechanical properties of the joints. (C) 2020 Acta Materialia Inc. Published by Elsevier Ltd.
引用
收藏
页码:12 / 16
页数:5
相关论文
共 50 条
  • [41] High and low cycle fatigue behavior of linear friction welded Ti-6Al-4V
    Stinville, J. C.
    Bridier, F.
    Ponsen, D.
    Wanjara, P.
    Bocher, P.
    INTERNATIONAL JOURNAL OF FATIGUE, 2015, 70 : 278 - 288
  • [42] Effects of size, geometry, and testing temperature on additively manufactured Ti-6Al-4V titanium alloy
    June, Daniel
    Mayeur, Jason R.
    Gradl, Paul
    Wessman, Andrew
    Hazeli, Kavan
    ADDITIVE MANUFACTURING, 2024, 80
  • [43] The evolution of microstructure of Ti-6Al-4V alloy during concurrent hot deformation and phase transformation
    He, Lijia
    Dehghan-Manshadi, A.
    Dippenaar, R. J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 549 : 163 - 167
  • [44] Friction Stir Lap Welding Ti-6Al-4V Alloy Using a Threaded Pin by Simulation and Experimental Investigation
    Liu, Zhenlei
    Yang, Kang
    Yue, Yumei
    Yan, Dejun
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (05) : 1279 - 1286
  • [45] Use of filler wire for laser welding of Ti-6Al-4V
    Kabir, A. S. H.
    Cao, X.
    Wanjara, P.
    Cuddy, J.
    Birur, A.
    Medraj, M.
    CANADIAN METALLURGICAL QUARTERLY, 2012, 51 (03) : 320 - 327
  • [46] Eliminating the tearing defect in Ti-6Al-4V alloy joint by back heating assisted friction stir welding
    Ji, Shude
    Li, Zhengwei
    Zhang, Liguo
    Wang, Yue
    MATERIALS LETTERS, 2017, 188 : 21 - 24
  • [47] Texture Evolution in Linear Friction Welded Ti-6Al-4V
    Dalgaard, E.
    Coghe, F.
    Rabet, L.
    Jahazi, M.
    Wanjara, P.
    Jonas, J. J.
    THERMEC 2009 SUPPLEMENT: 6TH INTERNATIONAL CONFERENCE ON PROCESSING & MANUFACTURING OF ADVANCED MATERIALS, 2010, 89-91 : 124 - +
  • [48] Nanostructural analysis of welded Ti-6Al-4V by linear friction welding applied for blisk assemblies
    Homma, T.
    Takano, H.
    Ozaki, T.
    MATERIALIA, 2019, 5
  • [49] Texture of friction stir welded Ti-6Al-4V alloy
    Zhou, Li
    Liu, Hui-jie
    Wu, Lin-zhi
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (02) : 368 - 372
  • [50] Fracture Toughness of Ti-6Al-4V and Ti-6Al-4V ELI Alloys Fabricated by Electron Beam Melting With Different Orientation and Positions
    Ninerola, Ruben
    Giner, Eugenio
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2025, 48 (05) : 2339 - 2353