MICROSTRUCTURE AND PROPERTIES DEGRADATION OF P/T 91, 92 STEELS WELDMENTS IN CREEP CONDITIONS

被引:9
作者
Falat, L. [1 ]
Homolova, V. [1 ]
Kepic, J. [1 ]
Svoboda, M. [2 ]
Vyrostkova, A. [1 ]
机构
[1] Slovak Acad Sci, Inst Mat Res, Kosice, Slovakia
[2] Acad Sci Czech Republ, Inst Phys Mat, Brno, Czech Republic
关键词
Dissimilar weldments; Microstructure; Creep behaviour; Phase composition; Thermodynamic calculations; WELDED-JOINTS; STRENGTH; BEHAVIOR; TEMPERATURE; TRANSITION; STABILITY;
D O I
10.2298/JMMB120701057F
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The studies were performed on dissimilar ferritic/austenitic weldments between 9Cr tempered martensitic steels of the grades either P/T 91 or 92 and unstabilised AISI316H austenitic steel. The welded joints were fabricated using the fusion welding by tungsten inert gas (TIG) method with Ni-based filler metal. Microstructural analyses were performed using light and electron microscopy. Microstructural gradient in heat-affected zone (HAZ) of 9Cr steels remained preserved during creep exposure. All weldments fractured by the type IV failure within their intercritical HAZ (ICHAZ) regions. The most remarkable microstructural change during creep was the precipitation of intermetallic Laves phase. Experimentally determined phases of the samples after creep exposure are in good agreement with equilibrium thermodynamic calculations.
引用
收藏
页码:461 / 469
页数:9
相关论文
共 20 条
[1]  
[Anonymous], ACTA METALL SLOVACA
[2]   TRANSITION-METAL JOINTS FOR STEAM-GENERATORS - AN OVERVIEW [J].
BHADURI, AK ;
VENKADESAN, S ;
RODRIGUEZ, P ;
MUKUNDA, PG .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 1994, 58 (03) :251-265
[3]  
Blach J, 2000, KOVOVE MATER, V38, P315
[4]   Creep properties and microstructural evolution of austenitic TEMPALOY steels [J].
Caminada, S. ;
Cumino, G. ;
Cipolla, L. ;
Venditti, D. ;
Di Gianfrancesco, A. ;
Minami, Y. ;
Ono, T. .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2010, 87 (06) :336-344
[5]  
Cerjak H, 2008, WOODHEAD PUBL MATER, P472, DOI 10.1533/9781845694012.2.472
[6]   ANALYSIS OF CREEP IN A WELDED P91 PRESSURE-VESSEL [J].
EGGELER, G ;
RAMTEKE, A ;
COLEMAN, M ;
CHEW, B ;
PETER, G ;
BURBLIES, A ;
HALD, J ;
JEFFEREY, C ;
RANTALA, J ;
DEWITTE, M ;
MOHRMANN, R .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 1994, 60 (03) :237-257
[7]   Microstructural stability and creep rupture strength of the martensitic steel P92 for advanced power plant [J].
Ennis, PJ ;
Zielinska-Lipiec, A ;
Wachter, O ;
CzyrskaFilemonowicz, A .
ACTA MATERIALIA, 1997, 45 (12) :4901-4907
[8]   The influence of PWHT regime on microstructure and creep rupture behaviour of dissimilar T92/TP316H ferritic/austenitic welded joints with Ni-based filler metal [J].
Falat, L. ;
Vyrostkova, A. ;
Svoboda, M. ;
Milkovic, O. .
KOVOVE MATERIALY-METALLIC MATERIALS, 2011, 49 (06) :417-426
[9]  
Igarashi M, 2008, WOODHEAD PUBL MATER, P539, DOI 10.1533/9781845694012.3.539
[10]   Transition from power-law to viscous creep behaviour of P-91 type heat-resistant steel [J].
Kloc, L ;
Sklenicka, V .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 234 :962-965