Carbon nanotubes prevent the coagulation at high shear rates of aqueous suspensions of equiaxed ceramic nanoparticles

被引:12
作者
Candelario, Victor M. [1 ]
Moreno, Rodrigo [2 ]
Ortiz, Angel L. [1 ]
机构
[1] Univ Extremadura, Dept Ingn Mecan Energet & Mat, Badajoz 06006, Spain
[2] CSIC, Inst Ceram & Vidrio, Madrid 28049, Spain
关键词
Aqueous colloidal processing; CNTs; Dispersion; Nanoceramics; Ceramic nanocomposites; ZIRCONIA; Y3AL5O12; BEHAVIOR; POWDERS;
D O I
10.1016/j.jeurceramsoc.2013.09.003
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Equiaxed ceramic nanoparticles and their mixtures are expected to exhibit shear-thinning behaviour when dispersed colloidally in aqueous media, whereas shear-thickening is the expectation for large aspect ratio phases such as, for example, carbon nanotubes (CNTs). Here, contrary experimental evidence is presented demonstrating the occurrence of severe coagulation at high shear rates in colloidally stable, semi-concentrated, aqueous suspensions of equiaxed SiC nanoparticles (major phase) mixed with equiaxed Y3Al5O12 nanoparticles (liquid-phase sintering additive), and how CNT addition prevents this coagulation if sufficient sonication is applied. It is also shown that although shear-thinning is the natural behaviour of the ceramic suspension up to moderate shear rates, coagulation is eventually a phenomenon inherent to the aqueous colloidal processing of these suspensions, with the critical shear rate for coagulation increasing and the rheopexy decreasing the better is the initial dispersion state achieved with the sonication. It is also shown that the critical shear rate for coagulation depends on the exact condition of shear rate increase, and that the re-sheared suspensions coagulate more significantly and at lower shear rates than the fresh suspensions. The mechanisms by which this coagulation occurs and is impeded by the CNTs are discussed, together with broader implications of these phenomena for the environmentally friendly processing of nanostructured ceramics and ceramic composites. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:555 / 563
页数:9
相关论文
共 30 条
[1]  
[Anonymous], 1998, An Introduction to Mechanical Properties of Ceramics, DOI DOI 10.1017/CBO9780511623103
[2]   Hardness degradation in liquid-phase-sintered SiC with prolonged sintering [J].
Borrero-Lopez, O. ;
Pajares, A. ;
Ortiz, A. L. ;
Guiberteau, F. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (11) :3359-3364
[3]   Colloidal behaviour of mullite powders produced by combustion synthesis [J].
Burgos-Montes, Olga ;
Moreno, Rodrigo .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (16) :4751-4757
[4]   Aqueous colloidal processing of SiC with Y3Al5O12 liquid-phase sintering additives [J].
Candelario, Victor M. ;
Nieto, Maria I. ;
Guiberteau, Fernando ;
Moreno, Rodrigo ;
Ortiz, Angel L. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (10) :1685-1694
[5]   Flash Sintering of Nanograin Zirconia in <5 s at 850°C [J].
Cologna, Marco ;
Rashkova, Boriana ;
Raj, Rishi .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (11) :3556-3559
[6]   Nanostructured materials: Basic concepts and microstructure [J].
Gleiter, H .
ACTA MATERIALIA, 2000, 48 (01) :1-29
[7]   INDUCTION PLASMA SYNTHESIS OF ULTRAFINE SIC POWDERS FROM SILICON AND CH4 [J].
GUO, JY ;
GITZHOFER, F ;
BOULOS, MI .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (22) :5589-5599
[8]   ARXPS STUDIES OF SIO2-SIC INTERFACES AND OXIDATION OF 6H SIC SINGLE-CRYSTAL SI-(001) AND C-(001)OVER-BAR SURFACES [J].
HORNETZ, B ;
MICHEL, HJ ;
HALBRITTER, J .
JOURNAL OF MATERIALS RESEARCH, 1994, 9 (12) :3088-3094
[9]   ULTRASONIC DISPERSION OF CERAMIC POWDERS [J].
JORGE, E ;
CHARTIER, T ;
BOCH, P .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (08) :2552-2554
[10]  
Larson R. G., 1999, The structure and rheology of complex fluids