Development and preliminary process design of beta-SiAlONs by the spark plasma sintering process

被引:2
作者
Letwaba, John [1 ]
Tlhabadira, Isaac [2 ]
Daniyan, Ilesanmi [3 ]
Daramola, Oluyemi [4 ]
Sadiku, Rotimi [1 ]
Seerane, Mandy [5 ]
机构
[1] Tshwane Univ Technol, Inst Nanoengn Res INER, Dept Chem Met & Mat Engn, Pretoria, South Africa
[2] Tshwane Univ Technol, Dept Mech Engn, ZA-0001 Pretoria, South Africa
[3] Tshwane Univ Technol, Dept Ind Engn, ZA-0001 Pretoria, South Africa
[4] Fed Univ Technol Akure, Dept Met & Mat Engn, Akure 340001, Nigeria
[5] CSIR, Adv Mat & Engn Mfg Cluster, POB 395, ZA-0001 Pretoria, South Africa
关键词
beta-SiAlON; Densification; Spark plasma sintering; Taguchi method; Wear rate; TRIBOLOGICAL BEHAVIOR; MECHANICAL-PROPERTIES; CERAMICS; WEAR; MICROSTRUCTURE; PERFORMANCE; FLUORINE; STEEL;
D O I
10.1007/s00170-020-05846-1
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
There is a need for improvement in the existing ceramic-based products such as the cutting tools due to the structural failures often experienced and the increasing operational costs. The development of refractory material (beta-SiAlON) with excellent properties, such as high strength and wear resistance, is vital in order to meet the service requirements. In this study, the spark plasma sintering (SPS) technique was used for the sintering of ceramic powders, namely, beta-Si3N4, AlN, Al2O3, and Y2O3, during the production of beta-SiAlON. The density, wear behavior, hardness, and microstructure of the beta-SiAlON produced were evaluated and optimized in relation to the effect of the sintering parameters in the following range: sintering temperature (1450-1750 degrees C), holding time (5-10 min), heating rate (50-100 degrees C/min), and thez-value (0-1.5). The approach is based on the Taguchi method which uses the signal-to-noise ratio and the analysis of variance to predict the optimum sintering parameters for maximum densification, superior wear resistance, and hardness of the resulting products. Thus, the properties of the sintered materials produced via the physical experimentations were measured as the products' quality characteristics and statistically analyzed to determine the contribution of each process parameter to the measured properties. The following are combination of optimum parameters which produced excellent mechanical properties: maximum density (1600 degrees C, 10 min, 75 degrees C/min, and 1.5), superior wear resistance (1600 degrees C, 7.5 min, 100 degrees C/min, and 0.75), and hardness (1600 degrees C, 5 min, 75 degrees C/min, and 1.5). Hence, work provides an insight into the process design and determination of the optimal combination of the process parameters for the development of beta-SiAlON with excellent mechanical properties via the SPS technique.
引用
收藏
页码:2603 / 2613
页数:11