Laser Cladding Process of 42CrMo Surface with Single-Pass

被引:4
作者
Cheng Wei [1 ]
Wu Meiping [1 ]
Tang Youhong [2 ]
Wang Hang [1 ]
Ye Xiu [1 ]
机构
[1] Jiangnan Univ, Jiangsu Prov Key Lab Adv Food Mfg Equipment & Tec, Wuxi 214122, Jiangsu, Peoples R China
[2] Suzhou Entry Exit Inspect & Quarantine Bur, Suzhou 215021, Jiangsu, Peoples R China
关键词
laser technique; laser cladding; single-pass; orthogonal test; dilution rate; microhardness;
D O I
10.3788/LOP56.041402
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The orthogonal test of laser cladding of Stellite6 coating on the 42CrMo alloy surface with single-pass is carried out and the influences of laser power, scanning speed, powder feeding rate and spot diameter on the dilution rate and microhardness of cladding layers as well as the interactive action among the main influencing factors arc analyzed. The results show that the laser power has the most significant influence on the dilution rate of cladding layer, while the scanning speed has the most obvious influence on the microhardness of cladding layer. The optimal process parameter combination is laser power of 1100 W, scanning speed of 8 mm.s(-1), powder feeding rate of 1.2- 1.4 rad.min(-1) and spot diameter of 3.7 mm from the comprehensive analysis of the dilution rate and microhardness of cladding layers.
引用
收藏
页数:8
相关论文
共 20 条
[1]  
Chen J., 2006, China Surf. Eng, V19, P50
[2]   激光功率对激光熔覆Ni包WC涂层组织与性能的影响 [J].
成诚 ;
赵剑峰 ;
田宗军 ;
冯君 ;
谢德巧 ;
肖猛 .
南京航空航天大学学报, 2016, 48 (06) :890-894
[3]   Effect of processing parameters of laser on microstructure and properties of cladding 42CrMo steel [J].
Cheng, Yan-hai ;
Cui, Ran ;
Wang, Hao-zheng ;
Han, Zheng-tong .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 96 (5-8) :1715-1724
[4]   Analysis of coaxial laser cladding processing conditions [J].
de Oliveira, U ;
Ocelík, V ;
De Hosson, JTM .
SURFACE & COATINGS TECHNOLOGY, 2005, 197 (2-3) :127-136
[5]  
Deng ZQ, 2017, CHINESE J LASERS, V44
[6]  
[黄凤晓 Huang Fengxiao], 2010, [热加工工艺, Hot Working Technology], V39, P119
[7]  
Huang FX., 2011, INVESTIGATION MICRO
[8]  
LI H, 2017, LASER OPTOELECTRONIC, V50
[9]  
LIANG X, 2016, HOT WORKING TECHNOLO, V45, P145
[10]  
Lin W S, 2008, HEAT TREATMENT TECHN, V29, P1