Indentation-induced microhardness changes in glasses: Possible fictive temperature increase caused by plastic deformation

被引:27
作者
Gross, T. M. [1 ]
Tomozawa, M. [1 ]
机构
[1] Rensselaer Polytech Inst, Sch Engn, Dept Mat Sci & Engn, Troy, NY 12180 USA
关键词
hardness; silica; silicates; soda-lime-silica;
D O I
10.1016/j.jnoncrysol.2008.05.042
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microhardness around a large indentation was measured for different types of glasses. In soda-lime silicate glass, a typical normal glass, the region in the immediate vicinity of the indentation was found to exhibit a lower hardness than the region far removed from the indentation. In silica glass, a typical anomalous glass, the region in the immediate vicinity of a large indentation was found to exhibit a higher hardness than the region far removed from the indentation. Asahi less brittle glass, an intermediate glass between normal and anomalous glasses, was found to exhibit little change in hardness in the vicinity of the large indentation. These findings can be explained by a deformation-induced fictive temperature increase leading to a lower hardness for soda-lime silicate glass and a higher hardness for silica glass. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:4056 / 4062
页数:7
相关论文
共 33 条
[1]  
[Anonymous], 2007, ANN BOOK ASTM STAND, V04.08
[2]   Plastic flow softening in a bulk metallic glass [J].
Bhowmick, R. ;
Raghavan, R. ;
Chattopadhyay, K. ;
Ramamurty, U. .
ACTA MATERIALIA, 2006, 54 (16) :4221-4228
[3]   Crack opening profiles of indentation cracks in normal and anomalous glasses [J].
Burghard, Z ;
Zimmermann, A ;
Rödel, J ;
Aldinger, F ;
Lawn, BR .
ACTA MATERIALIA, 2004, 52 (02) :293-297
[4]   MICROMECHANICS OF FLAW GROWTH IN STATIC FATIGUE - INFLUENCE OF RESIDUAL CONTACT STRESSES [J].
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (06) :322-325
[5]   ION IMPLANTATION-INDUCED AND RADIATION-INDUCED STRUCTURAL MODIFICATIONS IN AMORPHOUS SIO2 [J].
DEVINE, RAB .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1993, 152 (01) :50-58
[6]   Strain-hardening and residual stress effects in plastic zones around indentations [J].
Eriksson, CL ;
Larsson, PL ;
Rowciffe, DJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 340 (1-2) :193-203
[8]   SHEAR DEFORMATION UNDER PYRAMIDAL INDENTATIONS IN SODA-LIME GLASS [J].
HAGAN, JT .
JOURNAL OF MATERIALS SCIENCE, 1980, 15 (06) :1417-1424
[9]  
Hill R., 1950, The Mathematical Theory of Plasticity
[10]   MICROHARDNESS OF SIO2 GLASS IN VARIOUS ENVIRONMENTS [J].
HIRAO, K ;
TOMOZAWA, M .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1987, 70 (07) :497-502