Titanium film deposition by high-power impulse magnetron sputtering: Influence of pulse duration

被引:51
作者
Jing, F. J. [1 ]
Yin, T. L. [1 ]
Yukimura, K. [1 ,2 ]
Sun, H. [1 ]
Leng, Y. X. [1 ]
Huang, N. [1 ]
机构
[1] SW Jiaotong Univ, Minist Educ, Key Lab Adv Mat Technol, Chengdu 610031, Peoples R China
[2] Natl Inst Adv Ind Sci & Technol, Nanoelect Res Inst, Tsukuba, Ibaraki 3058568, Japan
关键词
HIPIMS; HPPMS; High-power glow; Glow; Magnetron; Deposition rate; Thermal spike; Target temperature; IMMERSION ION-IMPLANTATION; THIN-FILMS; STRESS RELIEF; ENERGY; DISCHARGE; TEMPERATURE; TEXTURE;
D O I
10.1016/j.vacuum.2012.06.003
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Surface modification with high-power glow discharges is a promising physical vapor deposition (PVD) technology for industrial usage. A metal ion density higher than 10(18) m(-3) can be obtained due to a high-power input in the plasma. In the present paper, titanium films were deposited on Si (100) substrates using high-power impulse magnetron sputtering (HIPIMS). The pulse duration was varied to investigate the deposition rate and the titanium film structure. The plasma source was an unbalanced magnetron sputtering (UBMS) discharge generation system. The deposition rate was correlated to the electrical characteristics. There was an instantaneous power threshold of approximately 36 kW to significantly increase the deposition rate by 4-5 times. The deposition rate increased linearly with respect to the average power until the average power reached 5.6 kW (about 30 W/cm(2) for a total area of the target), and an 83% increase of the deposition rate from the linear relationship was observed. The increase of the deposition rate was possibly closely related to the so-called thermal spike, where the target temperature increases due to a high power input to the target. The surface morphology and the crystalline structure of the films were studied for a variety of pulse durations, and the results were compared to the case of the direct-current magnetron sputtering (dcMS) process. The titanium films at an average power of 1.2 kW and a pulse duration of 50 mu s have a smaller crystalline size and a smoother surface than those at an average power of 825 W by dcMS. The crystal orientation (101) was dominated when the pulse duration was lengthened to 180 mu s, although the (002) orientation was dominant in dcMS. The crystal size and the surface roughness increased significantly when the pulse duration was increased from 50 mu s to 180 mu s in HIPIMS. The consumed power in the plasma by HIPIMS can be an important parameter for the crystal size and the structure. (C) 2012 Published by Elsevier Ltd.
引用
收藏
页码:2114 / 2119
页数:6
相关论文
共 50 条
  • [21] Bipolar high-power impulse magnetron sputtering synthesis of high-entropy carbides
    Hossain, Mohammad Delower
    Borman, Trent
    Mcllwaine, Nathaniel Seymour
    Maria, Jon-Paul
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2022, 105 (06) : 3862 - 3873
  • [22] Optimizing the deposition rate and ionized flux fraction by tuning the pulse length in high power impulse magnetron sputtering
    Rudolph, Martin
    Brenning, Nils
    Raadu, Michael A.
    Hajihoseini, Hamidreza
    Gudmundsson, Jon Tomas
    Anders, Andre
    Lundin, Daniel
    PLASMA SOURCES SCIENCE & TECHNOLOGY, 2020, 29 (05)
  • [23] Tungsten Oxide Thin Films for Electrochromic Applications: Pulse Width-Controlled Deposition by High-Power Impulse Magnetron Sputtering
    Najafi-Ashtiani, Hamed
    Bilek, Marcela M.
    Akhavan, Behnam
    ADVANCED ENGINEERING MATERIALS, 2024, 26 (06)
  • [24] Neutral gas simulation on the influence of rotating spokes on gas rarefaction in high-power impulse magnetron sputtering
    Trieschmann, Jan
    CONTRIBUTIONS TO PLASMA PHYSICS, 2018, 58 (05) : 394 - 403
  • [25] Influence of Voltage, Pulselength and Presence of a Reverse Polarized Pulse on an Argon-Gold Plasma during a High-Power Impulse Magnetron Sputtering Process
    Guljakow, Jurgen
    Lang, Walter
    PLASMA, 2023, 6 (04) : 680 - 698
  • [26] Microstructure and Platelet Adhesion Behavior of Titanium Oxide Films Synthesized by Reactive High-Power Pulse Magnetron Sputtering
    Yin, Tai-Lei
    Jing, Feng-Juan
    Sun, Hong
    Leng, Yongxiang
    Yukimura, Ken
    Huang, Nan
    IEEE TRANSACTIONS ON PLASMA SCIENCE, 2013, 41 (08) : 1837 - 1843
  • [27] Effect of the target power density on high-power impulse magnetron sputtering of copper
    Kozak, Tomas
    PLASMA SOURCES SCIENCE & TECHNOLOGY, 2012, 21 (02)
  • [28] Short-pulse high-power dual magnetron sputtering
    Oskirko, V. O.
    Zakharov, A. N.
    Semenov, V. A.
    Pavlov, A. P.
    Grenadyorov, A. S.
    Rabotkin, S. V.
    Solovyev, A. A.
    VACUUM, 2022, 200
  • [29] Gas Breakdown and Discharge Formation in High-Power Impulse Magnetron Sputtering
    Zuo, Xiao
    Chen, Rende
    Ke, Peiling
    Wang, Aiying
    IEEE TRANSACTIONS ON PLASMA SCIENCE, 2019, 47 (02) : 1215 - 1222
  • [30] Deposition of yttria-stabilized zirconia thin films by high power impulse magnetron sputtering and pulsed magnetron sputtering
    Sonderby, Steffen
    Aijaz, Asim
    Helmersson, Ulf
    Sarakinos, Kostas
    Eklund, Per
    SURFACE & COATINGS TECHNOLOGY, 2014, 240 : 1 - 6