Plastic deformation kinetics of electrodeposited Cu foil at low and intermediate homologous temperatures

被引:20
|
作者
Conrad, H [1 ]
Yang, D [1 ]
机构
[1] N Carolina State Univ, Dept Mat Sci & Engn, Raleigh, NC 27695 USA
关键词
grain size; grain boundary shear; dislocation pileup; cross slip; intersection of dislocations;
D O I
10.1007/s11664-002-0148-x
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The plastic deformation kinetics of electrodeposited (EP) Cu foil (grain size d=0.6 mum) were determined at 296-448 K and compared with those for vapor-deposited (V-P) foil (d=0.5 mum) tested at 77-473 K. The apparent activation volume v=kT partial derivative In (epsilon)over dot/partial derivativesigma for both materials exhibited a minimum at similar to350 K, and at this temperature, there occurred a marked increase in the temperature dependence of the flow stress sigma. The rate-controlling mechanism in both materials at T < 373 K appears to be grain boundary shear induced by dislocation pileups at the grain boundaries. The results at T = 373-473 K suggest that the dislocation pileups are relieved or prevented and that either cross slip or intersection of dislocations is rate controlling with stronger support for the latter. The determination of the rate-controlling mechanism at the higher temperatures is complicated by possible changes in defect structure due to thermal annealing, and therefore, the operative mechanism corresponds to a structure that may differ from the initial, as-deposited condition.
引用
收藏
页码:304 / 312
页数:9
相关论文
共 50 条
  • [41] Dynamic recovery and stress relaxation kinetics in crystals at low and high homologous temperatures
    Lubenets, SV
    PHYSICS OF THE SOLID STATE, 2002, 44 (01) : 75 - 81
  • [42] EFFECT OF COLD PLASTIC-DEFORMATION ON THE AUSTENITE INTERMEDIATE-RANGE DECOMPOSITION KINETICS
    LYUBCHENKO, AP
    SATANOVSKII, EA
    RUSSIAN METALLURGY, 1984, (06): : 145 - 148
  • [43] Effect of plastic deformation on the kinetics of the solid state reaction between Cu and Zn
    Angiolini, M
    Mazzone, G
    Montone, A
    Vittori-Antisari, M
    PHYSICAL REVIEW B, 1999, 59 (18) : 11733 - 11738
  • [44] Plastic deformation of nanometric single crystal silicon wire in AFM bending test at intermediate temperatures
    Namazu, T
    Isono, Y
    Tanaka, T
    JOURNAL OF MICROELECTROMECHANICAL SYSTEMS, 2002, 11 (02) : 125 - 135
  • [45] Deformation behavior of ecaped AZ31 mg alloy at low homologous temperatures
    Lee, H. S.
    Kim, D. W.
    Bang, W.
    Chang, Y. W.
    MAGNESIUM TECHNOLOGY 2007, 2007, : 163 - +
  • [46] Deformation Behavior and Precipitation Features in a Stretched Al-Cu Alloy at Intermediate Temperatures
    Lin, Y. C.
    Dong, Wen-Yong
    Zhu, Xu-Hao
    Wu, Qiao
    He, Ying-Jie
    MATERIALS, 2020, 13 (11)
  • [47] THE ABSENCE OF STEADY-STATE FLOW DURING LARGE STRAIN PLASTIC-DEFORMATION OF SOME FCC METALS AT LOW AND INTERMEDIATE TEMPERATURES
    HUGHES, DA
    NIX, WD
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (12): : 3013 - 3024
  • [48] THE FATIGUE LIFE AND PLASTIC-DEFORMATION CHARACTER OF COPPER AT LOW-TEMPERATURES
    YAKOVENKO, LF
    GRINBERG, NM
    INTERNATIONAL JOURNAL OF FATIGUE, 1983, 5 (04) : 239 - 243
  • [49] PLASTIC-DEFORMATION OF TERNARY COPPER-ALLOYS AT LOW-TEMPERATURES
    NIXON, WE
    MITCHELL, JW
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1973, 18 (03): : 445 - 445
  • [50] Plastic deformation of micrograined magnesium alloy AZ31 at low temperatures
    Isaev, N. V.
    Zabrodin, P. A.
    LOW TEMPERATURE PHYSICS, 2020, 46 (10) : 1044 - 1052