Room temperature demonstration of a sodium superionic conductor with grain conductivity in excess of 0.01 S cm-1 and its primary applications in symmetric battery cells
被引:157
作者:
Ma, Qianli
[1
,2
]
Tsai, Chih-Long
[1
,2
]
Wei, Xian-Kui
[3
]
Heggen, Marc
[3
]
Tietz, Frank
[1
,2
]
Irvine, John T. S.
[4
]
机构:
[1] Forschungszentrum Julich, Inst Energy & Climate Res Mat Synth & Proc IEK 1, D-52425 Julich, Germany
[2] Forschungszentrum Julich, Helmholtz Inst Munster, D-52425 Julich, Germany
[3] Forschungszentrum Julich, Peter Grunberg Inst, Ernst Ruska Ctr Microscopy & Spect Electrons, D-52425 Julich, Germany
[4] Univ St Andrews, Sch Chem, St Andrews KY16 9ST, Fife, Scotland
关键词:
SOLID-STATE BATTERIES;
IONIC-CONDUCTIVITY;
ELECTROLYTE;
TRANSPORT;
CHEMISTRY;
CATHODE;
NA;
D O I:
10.1039/c9ta00048h
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
The lack of suitable candidate electrolyte materials for practical application limits the development of all-solid-state Na-ion batteries. Na3+xZr2Si2+xP1-xO12 was the very first series of NASICONs discovered some 40 years ago; however, separation of bulk conductivity from total conductivity at room temperature is still problematic. It has been suggested that the effective Na-ion conductivity is approximate to 10(-4) S cm(-1) at room temperature for Na3+xZr2Si2+xP1-xO12 ceramics; however using a solution-assisted solid-state reaction for preparation of Na3+xZr2Si2+xP1-xO12, a total conductivity of 5 x 10(-3) S cm(-1) was achieved for Na3.4Zr2Si2.4P0.6O12 at 25 degrees C, higher than the values previously reported for polycrystalline Na-ion conductors. A bulk conductivity of 1.5 x 10(-2) S cm(-1) was revealed by high frequency impedance spectroscopy (up to 3 GHz) and verified by low temperature impedance spectroscopy (down to -100 degrees C) for Na3.4Zr2Si2.4P0.6O12 at 25 degrees C, indicating further the potential of increasing the related total conductivity. A Na/Na3.4Zr2Si2.4P0.6O12/Na symmetric cell showed low interface resistance and high cycling stability at room temperature. A full-ceramic cell was fabricated and tested at 28 degrees C with good cycling performance.