Hot deformation behavior and workability characteristic of a fine-grained Mg-8Sn-2Zn-2Al alloy with processing map

被引:79
作者
Cheng, Weili [1 ,2 ,3 ]
Bai, Yang [3 ]
Ma, Shichao [3 ]
Wang, Lifei [1 ,3 ]
Wang, Hongxia [1 ,3 ]
Yu, Hui [4 ]
机构
[1] Taiyuan Univ Technol, Shanxi Key Lab Adv Magnesium Based Mat, Taiyuan 030024, Shanxi, Peoples R China
[2] Taiyuan Univ Technol, Key Lab Interface Sci & Engn Adv Mat, Minist Educ, Taiyuan 030024, Shanxi, Peoples R China
[3] Taiyuan Univ Technol, Sch Mat Sci & Engn, Taiyuan 030024, Shanxi, Peoples R China
[4] Hebei Univ Technol, Sch Mat Sci & Engn, Tianjin 300132, Peoples R China
基金
山西省青年科学基金; 中国国家自然科学基金;
关键词
Mg-Sn based alloy; Hot deformation; Processing map; Dynamic recrystallization; DYNAMIC RECRYSTALLIZATION BEHAVIOR; MN-Y ALLOY; CONSTITUTIVE ANALYSIS; OPTIMUM PARAMETERS; WORKING; MICROSTRUCTURE; MECHANISMS; EVOLUTION; AL;
D O I
10.1016/j.jmst.2018.12.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The hot deformation behavior of a fine-grained Mg-8Sn-2Zn-2Al (TZA822, in wt%) alloy was investigated in the temperature range of 150-350 degrees C and the strain rate of 0.01-10 s(-1) employing thermomechanical simulator. In most of the cases, the material showed typical dynamic recrystallization (DRX) features i.e., a signal peak value followed by a gradual decrease or to reach a steady state. The work hardening rate was found to increase with decreasing temperature and increasing strain rate, while strain rates had great effects on work hardening behavior. Meanwhile, the constitutive analysis indicated that cross-slip of dislocations was likely to be the dominant deformation mechanism. In addition, the processing map at the strain of 0.1-0.7 showed two stability domains with high power dissipation efficiencies and the optimum hot working parameters for the studied alloy was determined to be 350 degrees C/0.01 s(-1) and 350 degrees C/10 s(-1), at which continuous DRX (CDRX) and discontinuous DRX (DDRX) as main softening mechanism. The instability regions occurred at 200-250 degrees C/10 s(-1) and the main flow instability mechanism was twinning and/or flow localization bands, which were prone to induce cracks and caused in-consistent mechanical properties of the alloy. (C) 2019 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:1198 / 1209
页数:12
相关论文
共 41 条
  • [1] Dynamic recrystallization behavior and hot workability of AZ41M magnesium alloy during hot deformation
    Cai, Zhiwei
    Chen, Fuxiao
    Ma, Fengjie
    Guo, Junqing
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 670 : 55 - 63
  • [2] Compressive deformation behavior of an indirect-extruded Mg-8Sn-1Al-1Zn alloy
    Cheng, Wei-li
    Que, Zhong-ping
    Zhang, Jin-shan
    Xu, Chun-xiang
    Liang, Wei
    You, Bong Sun
    Park, Sung Soo
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2013, 20 (01) : 49 - 56
  • [3] Strengthening Effect of Extruded Mg-8Sn-2Zn-2Al Alloy: Influence of Micro and Nano-Size Mg2Sn Precipitates
    Cheng, Weili
    Bai, Yang
    Wang, Lifei
    Wang, Hongxia
    Bian, Liping
    Yu, Hui
    [J]. MATERIALS, 2017, 10 (07):
  • [4] Optimum parameters and kinetic analysis for hot working of a homogenized Mg-8Sn-1Al-1Zn alloy
    Cheng, Weili
    Tian, Quanwei
    Yu, Hui
    You, Bong Sun
    Wang, Hongxia
    [J]. MATERIALS & DESIGN, 2015, 85 : 762 - 770
  • [5] Hot deformation behavior and processing maps of fine-grained SiCp/AZ91 composite
    Deng, Kun-kun
    Li, Jian-chao
    Xu, Fang-jun
    Nie, Kai-bo
    Liang, Wei
    [J]. MATERIALS & DESIGN, 2015, 67 : 72 - 81
  • [6] Dynamic recrystallization in AZ31 magnesium alloy
    Fatemi-Varzaneh, S. M.
    Zarei-Hanzaki, A.
    Beladi, H.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 456 (1-2): : 52 - 57
  • [7] Role of compression direction on recrystallization behavior and texture evolution during hot deformation of extruded ZK60 magnesium alloy
    Hadadzadeh, Amir
    Wells, Mary A.
    Shaha, Sugrib Kumar
    Jahed, Hamid
    Williams, Bruce W.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 702 : 274 - 289
  • [8] Annealing behaviour of Mg-3Al-1Zn alloy sheet obtained by a combination of high-temperature rolling and subsequent warm rolling
    Huang, Xinsheng
    Suzuki, Kazutaka
    Chino, Yasumasa
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (14) : 4854 - 4860
  • [9] Microstructure evolution and dynamic recrystallization behavior of a powder metallurgy Ti-22Al-25Nb alloy during hot compression
    Jia, Jianbo
    Yang, Yue
    Xu, Yan
    Xu, Bo
    Luo, Junting
    Zhang, Kaifeng
    [J]. MATERIALS CHARACTERIZATION, 2017, 123 : 198 - 206
  • [10] LAWS FOR WORK-HARDENING AND LOW-TEMPERATURE CREEP
    KOCKS, UF
    [J]. JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1976, 98 (01): : 76 - 85