Investigation of the corrosion behaviors of continuously hot-dip galvanizing Zn-Mg coating

被引:48
作者
Li, Baoping [1 ]
Dong, Anping [1 ]
Zhu, Guoliang [1 ]
Chu, Shuangjie [2 ]
Qian, Hongwei [2 ]
Hu, Chengjie [1 ]
Sun, Baode [1 ]
Wang, Jun [1 ]
机构
[1] Shanghai Jiao Tong Univ, State Lab Met Matrix Composites, Shanghai 200240, Peoples R China
[2] Baosteel Grp Corp, Shanghai 201900, Peoples R China
关键词
Zn-Mg coated steel; MgZn2; intermetallics; Corrosion behavior; Hot-dip galvanizing; ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY; ZINC-PLATED STEEL; COATED STEEL; MOLTEN-SALT; RESISTANCE; MAGNESIUM; SHEET; PVD; PERFORMANCE;
D O I
10.1016/j.surfcoat.2012.03.079
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Corrosion behaviors of continuously hot-dip galvanizing Zn-Mg (ZM) coating with 0.2 wt.% Al containing 1-3 wt.% Mg and Zn (GI) coating with 0.2 wt.% Al in an aerated and quiescent 5 wt.% NaCl solution were investigated. The linear polarization method was used to study corrosion path of Cl and ZM coatings. The experimental results show that the grain corrosion in the ZM coatings can be significantly inhibited by Mg after 24 hour immersion especially for the Zn coating containing 2 wt.% Mg. Localized corrosion occurred within Zn grains or Mg-rich regions when the Mg content is not 2 wt.%. The results of electrochemical impedance spectroscopy (EIS) also proved the results mentioned above. It was also found that Mg can significantly improve the adherence of the corrosion product layer and reduce surface cracks especially for a content of 2 wt.% Mg in the coating after 11 days of linear polarization treatment. The corrosion products of GI coating are as same as ZM coatings after the linear polarization treatment. The enhanced corrosion resistance of ZM coatings is mainly due to grain corrosion inhibition and strong adherence of corrosion products. (c) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:3989 / 3999
页数:11
相关论文
共 50 条
[31]   Contemporary use of Ni and Bi in hot-dip galvanizing [J].
Fratesi, R ;
Ruffini, N ;
Malavolta, M ;
Bellezze, T .
SURFACE & COATINGS TECHNOLOGY, 2002, 157 (01) :34-39
[32]   Factors shaping the appearance of hot-dip galvanizing coatings [J].
Janas, Zbigniew .
OCHRONA PRZED KOROZJA, 2009, 52 (10) :406-408
[33]   Production Process and Technology Development of Hot-dip Galvanizing [J].
Cai Xingfu ;
Huang Yongzhi ;
Li Yungang ;
Zhao Lina .
MATERIALS SCIENCE, CIVIL ENGINEERING AND ARCHITECTURE SCIENCE, MECHANICAL ENGINEERING AND MANUFACTURING TECHNOLOGY, PTS 1 AND 2, 2014, 488-489 :61-65
[34]   Hot-dip galvanizing - shield protecting from rust [J].
Jagiello, Wladyslaw .
OCHRONA PRZED KOROZJA, 2009, 52 (10) :402-405
[35]   Effect of Boron in AHSS on Coatability in Hot-Dip Galvanizing [J].
Tahara, Daisuke ;
Hoshino, Katsuya ;
Taira, Shoichiro .
CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2024, 23 (06) :503-509
[36]   Robustness margin of the hot-dip galvanizing control system [J].
Romero-Galván, G ;
García-Garza, LA ;
Pérez-Vargas, I .
CCA 2003: PROCEEDINGS OF 2003 IEEE CONFERENCE ON CONTROL APPLICATIONS, VOLS 1 AND 2, 2003, :1443-1447
[37]   A hot-dip self-passive zinc alloy coating to inhibit the galvanic corrosion of a Mg alloy [J].
Yang, Mingyu ;
Song, Guang-Ling .
CORROSION SCIENCE, 2025, 255
[38]   An Excellent Corrosion-Resistant Al-Si-Mg-Mn Hot-Dip Coating for Steel [J].
Pradhan, D. ;
Mondal, A. ;
Chakraborty, A. .
JOM, 2024, 76 (08) :4207-4222
[39]   Influence of strontium on electrochemical corrosion behavior of hot-dip galvanized coating [J].
Vagge, S. T. ;
Raja, V. S. .
SURFACE & COATINGS TECHNOLOGY, 2009, 203 (20-21) :3092-3098
[40]   Evaluation of the Corrosion Resistance of Hot-Dip Galvanized Magnesium and Aluminum Alloy Coating Using the Taguchi Method [J].
Kheirifard, Ramin ;
Ahmadi, Naghi Parvini ;
Aghaie, Ermia ;
Khezrloo, Amirreza ;
Tayebi, Morteza ;
Behnamian, Yashar .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (13) :6054-6071