Anodization of Aluminium using a fast two-step process

被引:27
|
作者
Ilango, Murugaiya Sridar [1 ]
Mutalikdesai, Amruta [1 ]
Ramasesha, Sheela K. [1 ]
机构
[1] Indian Inst Sci, Divecha Ctr Climate Change, Bangalore 560012, Karnataka, India
关键词
Anodization; phosphoric acid; anodization time; anodized aluminium oxide; aluminium; POROUS ALUMINA; OXIDE-FILMS; ARRAYS; FABRICATION; MEMBRANES; ACID; POROSITY; GROWTH;
D O I
10.1007/s12039-015-1006-8
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Ultra-fast two-step anodization method is developed for obtaining ordered nano-pores on aluminium (Al) foil. First anodization was carried out for 10 min, followed by 3 min of second anodization at high voltage (150 V) compared to previous reports of anodization times of 12 h (40-60 V). The pore dimensions on anodized alumina are 180 nm for pore diameter and 130 nm for inter-pore distance. It was evident that by increasing the anodization voltage to 150 V, the diameter of the pores formed was above 150 nm. The electrolyte and its temperature affect the shape and size of the pore formation. At lower anodization temperature, controlled pore formation was observed. The anodized samples were characterized using the field emission scanning electron microscope (FE-SEM) to determine the pore diameter and inter-pore distance. Using UV-Visible spectroscopy, the reflectance spectra of anodized samples were measured. The alumina (Al2O3) peaks were identified by x-ray diffraction (XRD) technique. The x-ray photo electron spectroscopy (XPS) analysis confirmed the Al 2p peak at 73.1 eV along with the oxygen O 1s at 530.9 eV and carbon traces C 1s at 283.6 eV.
引用
收藏
页码:153 / 158
页数:6
相关论文
共 50 条
  • [1] Anodization of Aluminium using a fast two-step process
    MURUGAIYA SRIDAR ILANGO
    AMRUTA MUTALIKDESAI
    SHEELA K RAMASESHA
    Journal of Chemical Sciences, 2016, 128 : 153 - 158
  • [2] Alumina nanostructures prepared by two-step anodization process
    Zhou Jian-hua
    He Jian-ping
    Zhao Gui-wang
    Zhang Chuan-xiang
    Zhao Ji-shuang
    Hu Huo-ping
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 (01) : 82 - 86
  • [3] Alumina nanostructures prepared by two-step anodization process
    周建华
    何建平
    赵桂网
    张传香
    赵继爽
    胡火平
    TransactionsofNonferrousMetalsSocietyofChina, 2007, (01) : 82 - 86
  • [4] Porous GaAs formed by a two-step anodization process
    Nagoya Inst of Technology, Nagoya, Japan
    J Cryst Growth, 3-4 (661-664):
  • [5] Porous GaAs formed by a two-step anodization process
    Hao, MS
    Uchida, H
    Shao, CL
    Soga, T
    Jimbo, T
    Umeno, M
    JOURNAL OF CRYSTAL GROWTH, 1997, 179 (3-4) : 661 - 664
  • [6] Fabrication of porous anodic alumina films by using two-step anodization process
    Pohl Institute of Solid State Physics, Tongji University, Shanghai 200092, China
    Yuanzineng Kexue Jishu, 2006, SUPPL. (61-66):
  • [7] Aluminium oxide nanowires synthesis from high purity aluminium films via two-step anodization
    Nazemi, Azadeh
    Najafian, Ahmad
    Sadjadi, Seyed Abolfazl Seyed
    SUPERLATTICES AND MICROSTRUCTURES, 2015, 81 : 1 - 6
  • [8] Synthesis of highly ordered nanopores on alumina by two-step anodization process
    Bwana, Nicholas N.
    JOURNAL OF NANOPARTICLE RESEARCH, 2008, 10 (02) : 313 - 319
  • [9] Synthesis of highly ordered nanopores on alumina by two-step anodization process
    Nicholas N. Bwana
    Journal of Nanoparticle Research, 2008, 10 : 313 - 319
  • [10] A comparative study of two-step anodization with one-step anodization at constant voltage
    Zeng, Huipeng
    Li, Chengyuan
    Dan, Yuxin
    Lu, Yishan
    Sun, Weidong
    Zhang, Shaoyu
    Song, Ye
    NANOTECHNOLOGY, 2023, 34 (06)