Kinetics of Spinel Formation and Growth during Dissolution of MgO in CaO-Al2O3-SiO2 Slag

被引:30
作者
Nightingale, S. A. [1 ]
Monaghan, B. J. [1 ]
机构
[1] Univ Wollongong, Fac Engn, Sch Mech Mat & Mechatron Mat Engn, Wollongong, NSW 2522, Australia
来源
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE | 2008年 / 39卷 / 05期
关键词
MgAl2O4; Slag Composition; Liquid Slag; Spinel Crystal; Spinel Formation;
D O I
10.1007/s11663-008-9186-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The formation and growth of MgAl2O4 spinel crystals on a single- crystal MgO substrate submerged in a 40 pct CaO, 40 pct SiO2, and 20 pct Al2O3 slag were directly observed using high-temperature microscopy. This showed that the crystals initially form on the MgO surface, but may break off and be carried out into the liquid slag. Still pictures extracted from digitally recorded images were used to measure the size of these crystals at 1420 degrees C, 1440 degrees C, and 1460 degrees C as a function of time. Growth of the crystals was found to follow the parabolic rate law, with rates increasing with temperature. An activation energy of 564 kJ mol(-1) was estimated from the experimental data. This was found to be comparable with previously published results from different types of experiments on spinel formation.
引用
收藏
页码:643 / 648
页数:6
相关论文
共 17 条
  • [1] Predicting lattice parameter as a function of cation disorder in MgAl2O4 spinel
    Ball, JA
    Pirzada, M
    Grimes, RW
    Zacate, MO
    Price, DW
    Uberuaga, BP
    [J]. JOURNAL OF PHYSICS-CONDENSED MATTER, 2005, 17 (48) : 7621 - 7631
  • [2] Callister W.D., 2007, MAT SCI ENG INTRO, P418
  • [3] Chen Y, 2005, CAN METALL QUART, V44, P323
  • [4] DAVIES RH, 1994, C APPL THERM SYNTH P, P371
  • [5] Goto K, 1997, J AM CERAM SOC, V80, P461
  • [6] KOFSTAD P, 1996, HIGH TEMPERATURE OXI, P306
  • [7] MCCLUNE WF, 1984, INT DIFFRACTION FILE, V4, P832
  • [8] Effect of changing slag composition on spinel inclusion dissolution
    Monaghan, B. J.
    Chen, L.
    [J]. IRONMAKING & STEELMAKING, 2006, 33 (04) : 323 - 330
  • [9] MONAGHAN BJ, 2004, P 7 INT C MOLT SLAGS, P598
  • [10] NAVAIS L, 1961, J AM CERAM SOC, V44, P434