Microstructure, residual stress, and fracture of sputtered TiN films

被引:115
作者
Zhang, Liqiang [1 ]
Yang, Huisheng [1 ]
Pang, Xiaolu [1 ]
Gao, Kewei [1 ]
Volinsky, Alex A. [2 ]
机构
[1] Univ Sci & Technol Beijing, Dept Mat Phys & Chem, Being 100083, Peoples R China
[2] Univ S Florida, Dept Mech Engn, Tampa, FL 33620 USA
关键词
TiN films; Residual stress; Hardness; Fracture toughness; POLYCRYSTALLINE THIN-FILMS; GRAIN-SIZE; MECHANICAL-PROPERTIES; INTRINSIC STRESSES; COATINGS; HARDNESS; GRADIENTS; GROWTH;
D O I
10.1016/j.surfcoat.2013.03.009
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Morphology, structure, residual stress, hardness, and fracture toughness of magnetron sputtered titanium nitride (TiN) thin films, deposited at 300 degrees C with a thickness in the 0.3- to 2-mu m range, were characterized. Film microstructure, the origin of residual stress, and its effect on the fracture toughness and hardness were analyzed. The grain size increased with the film thickness, with 1- to 2-mu m-thick films having high pore density. For the 2-mu m film, subgrains appeared at grain boundaries. X-ray diffraction showed (200) to (111) preferred orientation transition. The stress in the TiN films changed from highly compressive (-1.1 GPa) to tensile with the film thickness, reaching 0.68 GPa. Larger grain size, initial porosity, and subgrain generation are reasons for significant changes in the residual stress. Average hardness measured by nanoindentation is 23.2 +/- 0.6 GPa. The hardness of the films in compression is higher than in tension. Hardness variation with the film thickness is mainly due to the grain size and microstructure effects. The fracture toughness decreases with the film thickness, depending on the stress state and value. Compressive stress can significantly improve TIN film fracture toughness, while tensile stress seriously degrades it. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:120 / 125
页数:6
相关论文
共 24 条
  • [1] Role of underlayers in the development of evolutionary texture in polycrystalline thin films
    Adamik, M
    Barna, PB
    [J]. SURFACE & COATINGS TECHNOLOGY, 1996, 80 (1-2) : 109 - 112
  • [2] Effects of titanium-implanted pre-treatments on the residual stress of TiN coatings on high-speed steel substrates
    Chang, Chi-Lung
    Jao, Jui-Yun
    Ho, Wei-Yu
    Wang, Da-Yung
    [J]. SURFACE & COATINGS TECHNOLOGY, 2007, 201 (15) : 6702 - 6706
  • [3] CHARACTERISTICS OF NANOPHASE TIAL PRODUCED BY INERT-GAS CONDENSATION
    CHANG, H
    ALTSTETTER, CJ
    AVERBACK, RS
    [J]. JOURNAL OF MATERIALS RESEARCH, 1992, 7 (11) : 2962 - 2970
  • [4] GRAIN-GROWTH AND STRESS RELIEF IN THIN-FILMS
    CHAUDHAR.P
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1972, 9 (01): : 520 - &
  • [5] The origin of stresses in magnetron-sputtered thin films with zone T structures
    Daniel, R.
    Martinschitz, K. J.
    Keckes, J.
    Mitterer, C.
    [J]. ACTA MATERIALIA, 2010, 58 (07) : 2621 - 2633
  • [6] Effect of the substrate bias potential on crystalline grain size, intrinsic stress and hardness of vacuum arc evaporated TiN/c-Si coatings
    Espinoza-Beltrán, FJ
    Che-Soberanis, O
    García-González, L
    Morales-Hernández, J
    [J]. THIN SOLID FILMS, 2003, 437 (1-2) : 170 - 175
  • [7] Mechanics of compressive stress evolution during thin film growth
    Guduru, PR
    Chason, E
    Freund, LB
    [J]. JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2003, 51 (11-12) : 2127 - 2148
  • [8] Relationship between hardness and grain size in electrodeposited copper films
    Hakamada, Masataka
    Nakamoto, Yoshiaki
    Matsumoto, Hiroshi
    Iwasaki, Hajime
    Chen, Youqing
    Kusuda, Hiromu
    Mabuchi, Mamoru
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 457 (1-2): : 120 - 126
  • [9] A model for stresses, crack generation and fracture toughness calculation in scratched TiN-coated steel surfaces
    Holmberg, K
    Laukkanen, A
    Ronkainen, H
    Wallin, K
    Varjus, S
    [J]. WEAR, 2003, 254 (3-4) : 278 - 291
  • [10] Stress and strain in polycrystalline thin films
    Janssen, G. C. A. M.
    [J]. THIN SOLID FILMS, 2007, 515 (17) : 6654 - 6664