Experimental investigation and optimization of printing parameters of3Dprinted polyphenylene sulfide through response surface methodology

被引:60
作者
El Magri, Anouar [1 ,2 ]
El Mabrouk, Khalil [1 ]
Vaudreuil, Sebastien [1 ]
Ebn Touhami, Mohamed [2 ]
机构
[1] Euro Mediterranean Univ Fes, Euromed Engn Fac, Euromed Res Ctr, Eco Campus,Meknes Rd, Fes, Morocco
[2] Ibn Tofail Univ, Fac Sci, Lab Mat Engn & Environm Modeling & Applicat, Kenitra, Morocco
关键词
crystallization; glass transition; mechanical properties; thermal properties; FUSED FILAMENT FABRICATION; MECHANICAL-PROPERTIES; LAYER THICKNESS; POLY(PHENYLENE SULFIDE); FDM PROCESS; PERFORMANCE; PLA; IMPROVEMENT; PROPERTY; POLYMERS;
D O I
10.1002/app.49625
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Today fused filament fabrication is one of the most widely used additive manufacturing techniques to manufacture high performance materials. This method entails a complexity associated with the selection of their appropriate manufacturing parameters. Due to the potential to replace poly-ether-ether-ketone in many engineering components, polyphenylene sulfide (PPS) was selected in this study as a base material for 3D printing. Using central composite design and response surface methodology (RSM), nozzle temperature (T), printing speed (S), and layer thickness (L) were systematically studied to optimize the output responses namely Young's modulus, tensile strength, and degree of crystallinity. The results showed that the layer thickness was the most influential printing parameter on Young's modulus and degree of crystallinity. According to RSM, the optimum factor levels were achieved at 338 degrees C nozzle temperature, 30 mm/s printing speed, and 0.17 mm layer thickness. The optimized post printed PPS parts were then annealed at various temperatures to erase thermal residual stress generated during the printing process and to improve the degree of crystallinity of printed PPS's parts. Results showed that annealing parts at 200 degrees C for 1 hr improved significantly the thermal, structural, and tensile properties of printed PPS's parts.
引用
收藏
页数:13
相关论文
共 60 条
[1]   Anisotropic material properties of fused deposition modeling ABS [J].
Ahn, SH ;
Montero, M ;
Odell, D ;
Roundy, S ;
Wright, PK .
RAPID PROTOTYPING JOURNAL, 2002, 8 (04) :248-257
[2]  
Alafaghani A., 2017, OPEN J APPL SCI, V07, P291, DOI DOI 10.4236/OJAPPS.2017.76024
[3]   Critical parameters influencing the quality of prototypes in fused deposition modelling [J].
Anitha, R ;
Arunachalam, S ;
Radhakrishnan, P .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 118 (1-3) :385-388
[4]   Influence of annealing on the performance of short glass fiber-reinforced polyphenylene sulfide (PPS) composites [J].
Arici, A ;
Sinmazçelik, T ;
Çapan, L ;
Yilgör, I ;
Yilgör, E .
JOURNAL OF COMPOSITE MATERIALS, 2005, 39 (01) :21-33
[5]   Effect of printing layer thickness on water absorption and mechanical properties of 3D-printed wood/PLA composite materials [J].
Ayrilmis, Nadir ;
Kariz, Mirko ;
Kwon, Jin Heon ;
Kuzman, Manja Kitek .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 102 (5-8) :2195-2200
[6]   Effect of layer thickness on surface properties of 3D printed materials produced from wood flour/PLA filament [J].
Ayrilmis, Nadir .
POLYMER TESTING, 2018, 71 :163-166
[7]   SOLUBILITY CHARACTERISTICS OF POLY(ETHERETHERKETONE) AND POLY(PHENYLENE SULFIDE) [J].
BECK, HN .
JOURNAL OF APPLIED POLYMER SCIENCE, 1992, 45 (08) :1361-1366
[8]   Powder bed fusion of poly(phenylene sulfide) at bed temperatures significantly below melting [J].
Chatham, Camden A. ;
Long, Timothy E. ;
Williams, Christopher B. .
ADDITIVE MANUFACTURING, 2019, 28 :506-516
[9]  
Chirmeister C. G., 2019, ADDIT MANUF, V28, P152
[10]   Permanent magnets: Plugging the gap [J].
Coey, J. M. D. .
SCRIPTA MATERIALIA, 2012, 67 (06) :524-529