Evaluation method of sensitivity of hydrogen embrittlement for high strength bolts

被引:11
作者
Ham, Jong-Oh [1 ]
Jang, Yo-Han [1 ]
Lee, Geun-Pil [1 ]
Kim, Bok-Gi [1 ]
Rhee, Ki-Ho [2 ]
Cho, Chun-Kang [3 ]
机构
[1] Korea Testing & Res Inst, Metall Mat Team, Inchon 404817, South Korea
[2] POSCO Global R&D Ctr, Inchon 406840, South Korea
[3] Korea Agcy Technol & Stand, Mfg Ind Stand Div, Gwacheon Si 247723, Gyonggi Do, South Korea
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2013年 / 581卷
关键词
High strength bolt; Hydrogen embrittlement; Concentrated hydrogen; Intergranular fracture; WELD METAL; STEEL; SUSCEPTIBILITY; DEFORMATION;
D O I
10.1016/j.msea.2013.06.012
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, high strength bolts of 1100 MPa and 1300 MPa grades were charged with hydrogen to measure the sensitivity of hydrogen embrittlement (HE). Different levels of stress conditions based on various tensile stress and strain rates were applied. The bolts were then examined to see whether cracks were formed on the screw threads. The tensile stress and strain rate condition producing the most number of cracks on the screw thread of the bolt was decided as the most suitable test condition for the measurement of sensitivity of HE. For 1100 MPa grade high strength bolts, the most cracks were observed at the tensile stress ratio of 0.85 (load of 80 kN) and strain rate of 1.6 x 10E-5/s, while for 1300 MPa grades, the most cracks were observed at tensile stress ratio 0.87 (load of 100 kN) and strain rate of 1.6 x 10E-5/s. No cracks were found on the screw threads of bolt when the strain rate was increased over 8.3 x 10E-4/s. Crown Copyright (c) 2013 Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:83 / 89
页数:7
相关论文
共 17 条
[11]  
Nakamoto T., 2011, MAT SCI TECHNOLOGY, P1226
[12]   Effect of grain boundary ferrite on susceptibility to cold cracking in high-strength weld metal [J].
Seo, Jun Seok ;
Kim, Hee Jin ;
Ryoo, Hoi Soo .
METALS AND MATERIALS INTERNATIONAL, 2008, 14 (04) :515-522
[13]   Hydrogen Desorption Behavior of Pure Iron and Inconel 625 during Elastic and Plastic Deformation [J].
Shoda, Hiroki ;
Suzuki, Hiroshi ;
Takai, Kenichi ;
Hagihara, Yukito .
ISIJ INTERNATIONAL, 2010, 50 (01) :115-123
[14]   Lattice defects dominating hydrogen-related failure of metals [J].
Takai, K. ;
Shoda, H. ;
Suzuki, H. ;
Nagumo, M. .
ACTA MATERIALIA, 2008, 56 (18) :5158-5167
[15]   Absorption of Hydrogen in High-strength Low-alloy Steel during Tensile Deformation in Gaseous Hydrogen [J].
Takasawa, Koichi ;
Ishigaki, Ryoji ;
Wada, Yoru ;
Kayano, Rinzo .
ISIJ INTERNATIONAL, 2010, 50 (10) :1496-1502
[16]   Hydrogen degradation of a boron-bearing steel with 1050 and 1300MPa strength levels [J].
Wang, MQ ;
Akiyama, E ;
Tsuzaki, K .
SCRIPTA MATERIALIA, 2005, 52 (05) :403-408
[17]  
Yamasaki S., 1999, NIPPON STEEL TECH RE, V80, P50