The effect of manufacturing defects on the fatigue life of selective laser melted Ti-6Al-4V structures

被引:304
作者
Hu, Y. N. [1 ]
Wu, S. C. [1 ,2 ]
Withers, P. J. [2 ]
Zhang, J. [3 ]
Bao, H. Y. X. [1 ]
Fu, Y. N. [4 ]
Kang, G. Z. [1 ]
机构
[1] Southwest Jiaotong Univ, State Key Lab Tract Power, Chengdu 610031, Peoples R China
[2] Univ Manchester, Henry Royce Inst, Dept Mat, Manchester M13 9PL, Lancs, England
[3] AVIC Mfg Technol Inst, Beijing 100024, Peoples R China
[4] Chinese Acad Sci, Shanghai Adv Res Inst, Shanghai Synchrotron Radiat Facil SSRF, Shanghai 201204, Peoples R China
基金
英国工程与自然科学研究理事会; 欧洲研究理事会; 中国国家自然科学基金;
关键词
Defect tolerance method; Additive manufacturing; Fatigue crack initiation and growth; High cycle fatigue (HCF); Digital printing; MECHANICAL-PROPERTIES; POROSITY DEFECTS; PERFORMANCE; STRENGTH; ELECTRON; BEHAVIOR; ROUGHNESS; STRESS; DAMAGE;
D O I
10.1016/j.matdes.2020.108708
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The manufacturing defects introduced by selective laser melting typically lead to lower fatigue strength and a larger variation in fatigue life compared to conventionally manufactured structures. X-ray micro computed tomography (mu CT) is used to characterize the porosity and lack of fusion defects in terms of population, morphol-ogy, dimension and location. The defect size and location are combined with the NASA/FLACGRO (NASGRO) fatigue crack growth model to predict the likely fatigue life, in which an effective initial crack length is de fined using the cyclic plastic zone and the defect radius. An eXtended defect zone (XDZ) describing the propensity for local plasticity during fatigue around a defect has been shown through numerical analysis to be a good indicator of the ranking of the threat to fatigue caused by differently located manufacturing defects. This indicates that the effect of a defect, initial radius, r(0) , is likely to be pronounced when its center is within 2r(0) of the surface and maximal when it lies just beneath the surface. (C) 2020 The Author(s). Published by Elsevier Ltd.
引用
收藏
页数:10
相关论文
共 50 条
[31]   Controlling the tensile and fatigue properties of selective laser melted Ti-6Al-4V alloy by post treatment [J].
Su, Chenyu ;
Yu, Hanchen ;
Wang, Zemin ;
Yang, Jingjing ;
Zeng, Xiaoyan .
JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 857 (857)
[32]   Evaluation of Low Cycle Fatigue Performance of Selective Laser Melted Titanium Alloy Ti-6Al-4V [J].
Zhang, Peng ;
He, Allen Naihui ;
Liu, Fei ;
Zhang, Kaifei ;
Jiang, Junjie ;
Zhang, David Zhengwen .
METALS, 2019, 9 (10)
[33]   Laser-inherent porosity defects in additively manufactured Ti-6Al-4V implant: Formation, distribution, and effect on fatigue performance [J].
Aliyu, Abdul Azeez Abdu ;
Puncreobutr, Chedtha ;
Kuimalee, Surasak ;
Phetrattanarangsi, Thanawat ;
Boonchuduang, Thanachai ;
Taweekitikul, Pariwat ;
Panwisawas, Chinnapat ;
Shinjo, Junji ;
Lohwongwatana, Boonrat .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 :5121-5132
[34]   Fatigue performances of selective laser melted Ti-6Al-4V alloy: Influence of surface finishing, hot isostatic pressing and heat treatments [J].
Yu, Hanchen ;
Li, Fangzhi ;
Wang, Zemin ;
Zeng, Xiaoyan .
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 120 :175-183
[35]   Defect Induced Fatigue Behaviors of Selective Laser Melted Ti-6Al-4V via Synchrotron Radiation X-Ray Tomography [J].
Wu Zhengkai ;
Wu Shengchuan ;
Zhang Jie ;
Song Zhe ;
Hu Yanan ;
Kang Guozheng ;
Zhang Haiou .
ACTA METALLURGICA SINICA, 2019, 55 (07) :811-820
[36]   Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy [J].
Yang, Jingjing ;
Yu, Hanchen ;
Wang, Zemin ;
Zeng, Xiaoyan .
MATERIALS CHARACTERIZATION, 2017, 127 :137-145
[37]   Fatigue and biological properties of Ti-6Al-4V ELI cellular structures with variously arranged cubic cells made by selective laser melting [J].
Dallago, M. ;
Fontanari, V. ;
Torresani, E. ;
Leoni, M. ;
Pederzolli, C. ;
Potrich, C. ;
Benedetti, M. .
JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2018, 78 :381-394
[38]   Laser welding of electron beam melted Ti-6Al-4V to wrought Ti-6Al-4V: Effect of welding angle on microstructure and mechanical properties [J].
Sun, Y. Y. ;
Wang, P. ;
Lu, S. L. ;
Li, L. Q. ;
Nai, M. L. S. ;
Wei, J. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 782 :967-972
[39]   Fatigue Performance of Additively Manufactured Ti-6Al-4V: Surface Condition vs. Internal Defects [J].
Sun, Y. Y. ;
Lu, S. L. ;
Gulizia, S. ;
Oh, C. H. ;
Fraser, D. ;
Leary, M. ;
Qian, M. .
JOM, 2020, 72 (03) :1022-1030
[40]   Heat Treatment Degrading the Corrosion Resistance of Selective Laser Melted Ti-6Al-4V Alloy [J].
Dai, Nianwei ;
Zhang, Junxi ;
Chen, Yang ;
Zhang, Lai-Chang .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (07) :C428-C434