High temperature corrosion behavior of Cu-20Co-30Cr alloys with different grain size

被引:7
作者
Cao, Z. Q. [1 ]
Sun, H. J. [1 ]
Lu, J. [1 ]
Zhang, K. [1 ]
Sun, Y. [1 ]
机构
[1] Shenyang Normal Univ, Dept Chem, Shenyang 110034, Peoples R China
基金
中国国家自然科学基金;
关键词
High-temperature corrosion; Oxidation; Alloy; CU-CR ALLOYS; 1 ATM O-2; AIR OXIDATION; AL-ALLOYS; 1-ATM; 700-800-DEGREES-C; MODES;
D O I
10.1016/j.corsci.2013.11.025
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion behavior of Cu-20Co-30Cr alloys with different grain size was investigated at 700-900 degrees C in 0.1 MPa pure oxygen. The corrosion rates of fine-grained MACu-20Co-30Cr alloy are significantly lower than those of coarse-grained PMCu-20Co-30Cr alloy. PMCu-20Co-30Cr alloy forms the external scales of Cu oxides followed by an internal oxidation region containing alloy and a mixture of Cu, Co and Cr oxides as well as their complex oxides. MACu-20Co-30Cr alloy forms the continuous scales of chromia and a Cr-depleted layer occurs beneath the scales. The grain refinement is helpful to form the continuous scales of chromia in a Cu-Co-Cr alloy. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:184 / 190
页数:7
相关论文
共 30 条
[11]  
Kofstad P., 1988, HIGH TEMPERATURE COR
[12]  
Kosuge K., 2000, P 2000 POWD MET WORL
[13]   Anomalous Behavior of the Internal Oxidation of Dilute Cu-Ni Alloys Under 1 atm. O2 at 900 A°C [J].
Lu, L. Y. ;
Wang, S. ;
Gesmundo, F. ;
Niu, Y. .
OXIDATION OF METALS, 2011, 75 (5-6) :297-311
[14]  
Matecka J., 2012, CORROS SCI, V63, P287
[15]   The nature of the third-element effect in the oxidation of Fe-xCr-3 at.% Al alloys in 1 atm O2 at 1000 °C [J].
Niu, Y. ;
Wang, S. ;
Gao, F. ;
Zhang, Z. G. ;
Gesmundo, F. .
CORROSION SCIENCE, 2008, 50 (02) :345-356
[16]   The internal oxidation of ternary alloys. VIII: The transition from the internal to the external oxidation of the two most-reactive components under high-oxidant pressures [J].
Niu, Y. ;
Gesmundo, F. .
OXIDATION OF METALS, 2006, 65 (5-6) :329-355
[17]   High-temperature scaling of Cu-Al and Cu-Cr-Al alloys: An example of a non-classical third-element effect [J].
Niu, Y. ;
Wang, S. Y. ;
Gesmundo, F. .
OXIDATION OF METALS, 2006, 65 (5-6) :285-306
[18]   The third-element effect in the oxidation of Ni-xCr-7Al (x=0, 5, 10 15 at.%) alloys in 1 atm O2 at 900-1000 °C [J].
Niu, Y. ;
Zhang, X. J. ;
Wu, Y. ;
Gesmundo, F. .
CORROSION SCIENCE, 2006, 48 (12) :4020-4036
[19]   The air oxidation of two-phase Cu-Cr alloys at 700-900°C [J].
Niu, Y ;
Gesmundo, F ;
Viani, F ;
Douglass, DL .
OXIDATION OF METALS, 1997, 48 (5-6) :357-380
[20]   The air oxidation of two-phase Co-Cu alloys at 600-800°C [J].
Niu, Y ;
Song, J ;
Gesmundo, F ;
Farne, G ;
Fu, G ;
Zeng, C .
CORROSION SCIENCE, 2000, 42 (05) :799-815