Performance enhancements of die casting tools trough PVD nanocoatings

被引:14
作者
Rosso, M. [1 ]
Ugues, D. [1 ]
Torres, E. [1 ]
Perucca, M. [2 ]
Kapranos, P. [3 ]
机构
[1] Politecn Torino, I-10129 Turin, Italy
[2] Clean NT Lab, I-10144 Turin, Italy
[3] Univ Sheffield, Sheffield S1 3JD, S Yorkshire, England
关键词
PVD ceramic coatings; aluminium die casting; washout; soldering; modulated PVD composition;
D O I
10.1007/s12289-008-0131-z
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Wear and failure of die casting dies involve a complex interaction between various mechanisms. The most important wear and failure modes are summarized as follows: (i) the so-called washout damages on working die surfaces are attributed to erosion, corrosion and soldering; (ii) thermal fatigue is the most important failure mode in die casting. The sector of surface thin PVD coatings is constantly enhancing in order to meet the increasing demand for improved performances of tooling. Advanced PVD coatings are designed to withstand severe mechanical and thermal stress conditions. A CrAlSiN nanostructured coating system was deposited on the base material, modulating the chemical composition so as to increase either the chromium or the aluminium-silicon content. Then, another set of specimens was subjected to a cyclic immersion program in a molten aluminium bath. The washout signs were detected and monitored in function of the increasing number of cycles.
引用
收藏
页码:1259 / 1262
页数:4
相关论文
共 7 条
[1]   Adhesion of carbon nitride thin films on tool steel [J].
Chowdhury, AKMS ;
Cameron, DC ;
Hashmi, MSJ .
SURFACE & COATINGS TECHNOLOGY, 1999, 116 :46-53
[2]  
Joshi V., 2002, P 6 INT C TOOL KARLS, P809
[3]   Application of hard coatings in aluminium die casting -: soldering, erosion and thermal fatigue behaviour [J].
Mitterer, C ;
Holler, F ;
Üstel, F ;
Heim, D .
SURFACE & COATINGS TECHNOLOGY, 2000, 125 (1-3) :233-239
[4]  
Mitterer C., 1999, 5 INT C TOOL LEOB, P357
[5]  
Mitterer C., 1999, SURFACE COATINGS TEC, V116-119, P530
[6]  
Silipigni A., 2004, P 2 INT C HIGH TECH, P155
[7]   Indentation hardness evaluation of cathodic are deposited thin hard coatings [J].
Tuck, JR ;
Korsunsky, AM ;
Bhat, DG ;
Bull, SJ .
SURFACE & COATINGS TECHNOLOGY, 2001, 139 (01) :63-74