Mechanical behavior of a Si-Ti-C-O fiber-bonded ceramic material

被引:2
作者
Zawada, LP [1 ]
Ishikawa, T
机构
[1] AFRL, MLLN, Wright Patterson AFB, OH 45433 USA
[2] Ube Ind, Yamaguchi 775, Japan
来源
HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES III | 1999年 / 164-1卷
关键词
tensile; fatigue; intermediate temperature embrittlement; oxidation;
D O I
10.4028/www.scientific.net/KEM.164-165.245
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ceramic fibers of Si-Ti-C-O were heat treated in air to produce an oxide layer on the surface, and then hot pressed to produce a dense body containing a fiber volume fraction of approximately 80%. Longitudinal tensile data was generated at 23 degrees C, 1000 degrees, and 1150 degrees C to characterize the stress-strain behavior. Results revealed that at 1150 degrees C this composite experienced a reduction in strength of 28%. Fatigue tests at 1000 degrees C and 1150 degrees C were conducted to evaluate the high temperature durability of this composite. The fatigue testing revealed that this system had a similar stress run out level for both temperatures, but exhibited evidence of high temperature oxidation and intermediate temperature embrittlement.
引用
收藏
页码:245 / 248
页数:4
相关论文
共 50 条
  • [41] Oxidation behavior of different La2O3-content modified SiC ceramic at 1700 °C
    Xie, Wei
    Fu, Qiangang
    Cheng, Chunyu
    Yan, Ningning
    CERAMICS INTERNATIONAL, 2021, 47 (08) : 11560 - 11567
  • [42] Mechanical properties of two types of Al2O3/TiC ceramic cutting tool material at room and elevated temperatures
    Cheng, Moli
    Liu, Hanlian
    Zhao, Bin
    Huang, Chuanzhen
    Yao, Peng
    Wang, Bo
    CERAMICS INTERNATIONAL, 2017, 43 (16) : 13869 - 13874
  • [43] Comparison of microstructure and ablation behavior of Si-Mo-Ti/Al/Zr infiltrated C/C composites prepared at different infiltration temperature
    Hao, Zhenhua
    Sun, Wei
    Xiong, Xiang
    Xu, Yonglong
    Chang, Yabin
    Peng, Zheng
    Chen, Zhaoke
    Wang, Yalei
    CERAMICS INTERNATIONAL, 2017, 43 (02) : 2765 - 2773
  • [44] Microstructure and mechanical properties of hot pressed Mo-Cr-Si-Ti in-situ composite, and oxidation behavior with silicide coatings
    Paul, Bhaskar
    Majumdar, Sanjib
    Suri, A. K.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2013, 38 : 26 - 34
  • [45] Hot corrosion behavior of Yb2Si2O7 ceramic under NaVO3 salt attack
    Zhang, Yongqiu
    Zou, Binglin
    Cai, Xiaolong
    Wang, Ying
    Cao, Xueqiang
    CERAMICS INTERNATIONAL, 2020, 46 (03) : 2618 - 2623
  • [46] High Temperature Flexural, Tensile Strength and Oxidation Behavior of Ti3SiC2 Ceramic at 900°C-1300°C in Ambient Air
    He, R.
    Zhou, Z.
    Qu, Z.
    Cheng, X.
    JOURNAL OF TESTING AND EVALUATION, 2017, 45 (04) : 1150 - 1158
  • [47] Cyclic-Oxidation Behavior of Ti3Al0.7Si0.3C2 Compounds Between 900 and 1100 A°C in Air
    Nguyen, Thuan Dinh
    Park, Sang Whan
    Lee, Dong Bok
    OXIDATION OF METALS, 2009, 72 (5-6): : 299 - 309
  • [48] Cyclic-Oxidation Behavior of Ti3Al0.7Si0.3C2 Compounds Between 900 and 1100 °C in Air
    Thuan Dinh Nguyen
    Sang Whan Park
    Dong Bok Lee
    Oxidation of Metals, 2009, 72 : 299 - 309
  • [49] Oxidation and Tribological Behavior of Ti-B-C-N-Si Nanocomposite Films Deposited by Pulsed Unbalanced Magnetron Sputtering
    Jang, Jaeho
    Heo, Sungbo
    Kim, Wang Ryeol
    Kim, Jun-Ho
    Nam, Dae-Geun
    Kim, Kwang Ho
    Park, Ikmin
    Park, In-Wook
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2018, 18 (03) : 2100 - 2103
  • [50] Oxidation behavior of Ti0.2Zr0.2Hf0.2Nb0.2Ta0.2C-Mx C (M = Ti, Zr, Hf, Nb, Ta) composite ceramic at high temperature
    Xu, Shuai
    Wang, Tao
    Wang, Xingang
    Wu, Lu
    Fang, Zhongqiang
    Ge, Fangfang
    Meng, Xuan
    Liao, Qing
    Wei, Jinchun
    Li, Bingsheng
    CHINESE PHYSICS B, 2023, 32 (06)