Toughening by SiC Nanowires in a Dense SiC-Si Ceramic Coating for Oxidation Protection of C/C Composites

被引:35
作者
Chu, Yanhui [1 ]
Li, Hejun [1 ]
Fu, Qiangang [1 ]
Qi, Lehua [2 ]
Zou, Xu [1 ]
机构
[1] Northwestern Polytech Univ, Carbon Carbon Composites Res Ctr, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Northwestern Polytech Univ, Sch Mechatron Engn, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
CARBON/CARBON COMPOSITES; IN-SITU; MECHANICAL-PROPERTIES; ROOM-TEMPERATURE; FRACTURE; MICROSTRUCTURE; PLASTICITY; LAYER;
D O I
10.1111/j.1551-2916.2012.05412.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A dense oxidation protective SiC-Si ceramic coating with well-dispersion SiC nanowires was prepared on carbon/carbon (C/C) composites using a two-step technique consisting of chemical vapor deposition and hot-pressing reactive sintering. The results showed that the toughness and thermal shock resistance of the coating were dramatically improved, resulting in an excellent oxidation protection for the coated C/C composites, which is attributed primarily to the toughening effects of SiC nanowires in the coating including two special energy dissipation mechanisms involving the super-plasticity deformation of SiC nanowires and the plastic fracture at the interface of the nanowire-matrix, except for nanowire pullout, nanowire bridging, and microcrack deflection. More importantly, a novel oxidation protective failure mechanism of the coated C/C composites revealed that the presence of Al3+ in the coating, damaged the network structure of SiO2 glass and resulted in the slight oxidation of C/C composites.
引用
收藏
页码:3691 / 3697
页数:7
相关论文
共 36 条
[1]   Carbon-nanotube-reinforeed polymer-derived ceramic composites [J].
An, LN ;
Xu, WX ;
Rajagopalan, S ;
Wang, CM ;
Wang, H ;
Fan, Y ;
Zhang, LG ;
Jiang, DP ;
Kapat, J ;
Chow, L ;
Guo, BH ;
Liang, J ;
Vaidyanathan, R .
ADVANCED MATERIALS, 2004, 16 (22) :2036-+
[2]   In situ carbon nanotube reinforcements in a plasma-sprayed aluminum oxide nanocomposite coating [J].
Balani, K. ;
Zhang, T. ;
Karakoti, A. ;
Li, W. Z. ;
Seal, S. ;
Agarwal, A. .
ACTA MATERIALIA, 2008, 56 (03) :571-579
[3]  
Cantera EL, 1998, MATER LETT, V37, P201, DOI 10.1016/S0167-577X(98)00092-5
[4]   EFFECT OF INTERFACES ON THE PROPERTIES OF FIBER-REINFORCED CERAMICS [J].
CAO, HC ;
BISCHOFF, E ;
SBAIZERO, O ;
RUHLE, M ;
EVANS, AG ;
MARSHALL, DB ;
BRENNAN, JJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (06) :1691-1699
[5]   Low-temperature densification of zirconium diboride ceramics by reactive hot pressing [J].
Chamberlain, Adam L. ;
Fahrenholtz, William G. ;
Hilmas, Gregory E. .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (12) :3638-3645
[6]   Oxidation protection of C/C composites with a multilayer coating of SiC and Si plus SiC plus SiC nanowires [J].
Chu Yanhui ;
Li Hejun ;
Fu Qiangang ;
Wang Haipeng ;
Hou Xianghui ;
Zou Xu ;
Shang Gunan .
CARBON, 2012, 50 (03) :1280-1288
[7]   Effect of SiC Nanowires on the Mechanical and Oxidation Protective Ability of SiC Coating for C/C Composites [J].
Chu Yanhui ;
Fu Qiangang ;
Li Hejun ;
Shi Xiaohong ;
Li Kezhi ;
Wen Xue ;
Shang Gunan .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (02) :739-745
[8]   Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C [J].
Chu, Yanhui ;
Fu, Qiangang ;
Li, Hejun ;
Li, Kezhi ;
Zou, Xu ;
Gu, Caige .
CORROSION SCIENCE, 2011, 53 (09) :3048-3053
[9]   METAL-OXIDE INTERFACES [J].
ERNST, F .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 1995, 14 (03) :97-156
[10]   Multilayer oxidation protective coating for C/C composites from room temperature to 1500 °C [J].
Fu Qian-Cang ;
Li He-Jun ;
Wang Yong-Jie ;
Li Ke-Zhi ;
Tao Jun .
SURFACE & COATINGS TECHNOLOGY, 2010, 204 (11) :1831-1835