Effects of temperature and molecular weight on dissolution of cellulose in NaOH/urea aqueous solution

被引:217
|
作者
Qi, Haisong [1 ]
Chang, Chunyu [1 ]
Zhang, Lina [1 ]
机构
[1] Wuhan Univ, Dept Chem, Wuhan 430072, Peoples R China
基金
国家高技术研究发展计划(863计划); 中国国家自然科学基金;
关键词
Cellulose; Solubility; Temperature; Molecular weight; Crystallinity;
D O I
10.1007/s10570-008-9230-8
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
Dissolution of cellulose having different viscosity-average molecular weight (M-eta) in 7 wt% NaOH/12 wt%urea aqueous solution at temperature from 60 to -12.6 degrees C was investigated with optical microscope, viscosity measurements and wide X-ray diffraction (WXRD). The solubility (S-a) of cellulose in NaOH/urea aqueous solution strongly depended on the temperature, and molecular weight. Their S-a values increased with a decrease in temperature, and cellulose having M-eta below 10.0 x 10(4) could be dissolved completely in NaOH/urea aqueous solution pre-cooled to -12.6 degrees C. The activation energy of dissolution (E-a,E-s) of the cellulose dissolution was a negative value, suggesting that the cellulose solution state had lower enthalpy than the solid cellulose. The cellulose concentration in this system increased with a decrease of M-eta to achieve about 8 wt% for M-eta of 3.1 x 10(4). Moreover, cellulose having 12.7 x 10(4) could be dissolved completely in the solvent pre-cooled to -12.6 degrees C as its crystallinity (chi(c)) decreased from 0.62 to 0.53. We could improve the solubility of cellulose in NaOH/urea aqueous system by changing M-eta, chi(c) and temperature. In addition, the zero-shear viscosity (eta(0)) at 0 degrees C for the 4 wt% cellulose solution increased rapidly with an increase of M-eta, as a result of the enhancement of the aggregation and entanglement for the relatively long chains.
引用
收藏
页码:779 / 787
页数:9
相关论文
共 50 条
  • [41] Dissolution of Cellulose in Aqueous NaOH Solutions
    A. Isogai
    R. H. Atalla
    Cellulose, 1998, 5 : 309 - 319
  • [42] Dissolution of cellulose in aqueous NaOH solutions
    Isogai, A
    Atalla, RH
    CELLULOSE, 1998, 5 (04) : 309 - 319
  • [43] Glycerin/NaOH Aqueous Solution as a Green Solvent System for Dissolution of Cellulose
    Li, Ke
    Yang, Huiyu
    Jiang, Lang
    Liu, Xin
    Lang, Peng
    Deng, Bo
    Li, Na
    Xu, Weilin
    POLYMERS, 2020, 12 (08)
  • [44] Synthesis of amphoteric cellulose in aqueous NaOH/urea solution in one pot
    Song, Junlong
    He, Aijian
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2014, 247
  • [45] Cellulose microporous membranes prepared from NaOH/urea aqueous solution
    Zhou, JP
    Zhang, L
    Cai, J
    Shu, H
    JOURNAL OF MEMBRANE SCIENCE, 2002, 210 (01) : 77 - 90
  • [46] Hydrogels prepared from unsubstituted cellulose in NaOH/Urea aqueous solution
    Zhou, Jinping
    Chang, Chunyu
    Zhang, Ruping
    Zhang, Lina
    MACROMOLECULAR BIOSCIENCE, 2007, 7 (06) : 804 - 809
  • [47] Novel fibers prepared from cellulose in NaOH/urea aqueous solution
    Cai, J
    Zhang, LN
    Zhou, JP
    Li, H
    Chen, H
    Jin, HM
    MACROMOLECULAR RAPID COMMUNICATIONS, 2004, 25 (17) : 1558 - 1562
  • [48] Quantitative NMR investigation on the low-temperature dissolution mechanism of chitin in NaOH/urea aqueous solution
    Ru, Geying
    Luo, Huan
    Liang, Xinmiao
    Wang, Liying
    Liu, Chaoyang
    Feng, Jiwen
    CELLULOSE, 2015, 22 (04) : 2221 - 2229
  • [49] Quantitative NMR investigation on the low-temperature dissolution mechanism of chitin in NaOH/urea aqueous solution
    Geying Ru
    Huan Luo
    Xinmiao Liang
    Liying Wang
    Chaoyang Liu
    Jiwen Feng
    Cellulose, 2015, 22 : 2221 - 2229
  • [50] Effects of coagulants on porous structure of membranes prepared from cellulose in NaOH/urea aqueous solution
    Mao, Yuan
    Zhou, Jinping
    Cai, Jie
    Zhang, Lina
    JOURNAL OF MEMBRANE SCIENCE, 2006, 279 (1-2) : 246 - 255