Exfoliation Corrosion of HE.15 Aluminium Alloy

被引:1
作者
Hutchings, F. R. [1 ]
机构
[1] British Engine Insurance Ltd, Manchester, England
关键词
Aging (artificial); Bars; Extrusions; Protective coatings; HE.15; Exfoliation corrosion;
D O I
10.1007/s11668-022-01539-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Aluminum alloy BS.1476-HE.15 by virtue of its high strength and low density finds application in the form of bars or sections for cranes, bridges, and other such structures where a reduction in dead weight load and inertia stresses is advantageous. Bars and sections in H.15 alloy are mostly produced by extrusion. Some material processed this way has been prone to exfoliation corrosion. Extended aging for 24 h at a temperature of 185 degrees C (365 degrees F) virtually suppresses the tendency for exfoliation corrosion to develop. Also, the use of a sprayed coating, either of aluminum or Al-1Zn alloy, was effective in halting and preventing this form of attack. While alarming, the appearance of exfoliation corrosion provides a valuable warning to the engineer or inspector before a severe weakening of the particular sections has occurred.
引用
收藏
页码:2443 / 2446
页数:4
相关论文
共 11 条
  • [1] [Anonymous], 1963, CHEM IND-LONDON, P359
  • [2] [Anonymous], 2002, ASM HDB, V11, P761, DOI [10.31399/asm.hb.v11.a0003548, DOI 10.31399/ASM.HB.V11.A0003548]
  • [3] BELL WA, 1961, J I MET, V89, P464
  • [4] Budd, CORROSION-US, DOI [10.5006/0010-9312-18.5.197, DOI 10.5006/0010-9312-18.5.197]
  • [5] CARTER VE, 1961, J I MET, V89, P472
  • [6] Liddiard EAG., 1953, J I MET, V82, P377
  • [7] Liddiard EAG., 1960, J I MET, V61, P423
  • [8] METCALFE GJ, 1953, J I MET, V81, P269
  • [9] ROBERTSON WD, 1946, T AM I MIN MET ENG, V166, P216
  • [10] ROMANS HB, 1969, MATER RES STANDARD, V9, P31