共 26 条
Carbon dioxide reforming of methane over Ni catalysts prepared from Ni-Mg-Al layered double hydroxides: Influence of Ni loadings
被引:88
作者:
Lin, Xingyi
[1
]
Li, Rule
[1
]
Lu, Miaomiao
[1
]
Chen, Chongqi
[1
]
Li, Dalin
[1
]
Zhan, Yingying
[1
]
Jiang, Lilong
[1
]
机构:
[1] Fuzhou Univ, Sch Chem Engn, NERC CFC, Fuzhou 350002, Fujian, Peoples R China
来源:
基金:
国家高技术研究发展计划(863计划);
关键词:
Methane;
Carbon dioxide;
Synthesis gas;
Ni catalyst;
Layered double hydroxides;
HYDROGEN-PRODUCTION;
COKE FORMATION;
CH4;
STABILITY;
SYNGAS;
D O I:
10.1016/j.fuel.2015.09.021
中图分类号:
TE [石油、天然气工业];
TK [能源与动力工程];
学科分类号:
0807 ;
0820 ;
摘要:
A series of supported Ni/Mg/Al catalysts with Ni loadings of 3-18 wt% were prepared from Ni-Mg-Al layered double hydroxides and tested for the CH4-CO2 reforming. The influence of Ni loading on the catalyst activity and stability was studied. It is found that the catalyst activity increased with increasing the Ni loading. However, the CO disproportionation became significant as the Ni loading increased. The long-term stability of the Ni/Mg/Al catalysts was influenced by the Ni loading as well as the reaction temperature. At a high temperature of 1023 K, the catalyst stability increased with increasing the Ni loading, whereas it decreased with increasing the Ni loading at a low temperature of 873 K. The characterization on the spent Ni/Mg/Al catalysts showed that the sintering of Ni metal particles increased with increasing the Ni loading, and it became more severe at 873 K than at 1023 K. On the other hand, the coke deposition at 1023 K tended to decrease with increasing the Ni loading, and an opposite tendency was observed at 873 K. The coke deposition particularly the encapsulating carbon was considered to be responsible for the catalyst deactivation. A Ni loading of 12 wt% would be suitable for the Ni/Mg/Al catalyst considering its high activity, good stability, and less coke deposition at high temperature. (C) 2015 Elsevier Ltd. All rights reserved.