Preliminary electrochemical testing of some Zr-Ti alloys in 0.9% NaCl solution

被引:28
作者
Chelariu, R. [1 ]
Mareci, D. [2 ]
Munteanu, C. [3 ]
机构
[1] Gheorghe Asachi Tech Univ Iasi, Fac Mat Sci & Engn, Iasi 700050, Romania
[2] Gheorghe Asachi Tech Univ Iasi, Fac Chem Engn & Environm Protect, Iasi 700050, Romania
[3] Gheorghe Asachi Tech Univ Iasi, Fac Mech Engn, Iasi 700050, Romania
来源
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION | 2013年 / 64卷 / 07期
关键词
corrosion; EIS; localized corrosion; saline solution; ZrTi alloys; IN-VITRO CORROSION; MECHANICAL-PROPERTIES; LOCALIZED CORROSION; BIOMEDICAL ALLOY; PASSIVE STATE; BEHAVIOR; EIS; MICROSTRUCTURE; GRINDABILITY; STABILITY;
D O I
10.1002/maco.201206717
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study is to investigate the corrosion behaviour of three ZrTi alloys (denoted with Zr5Ti, Zr25Ti, and Zr45Ti) in 0.9% NaCl solution. For comparison, cp-Ti was also investigated. In order to study the localized corrosion resistance and corrosion behavior at open circuit potential versus time, the open circuit potential (E-OC) was recorded, and the cyclic potentiodynamic polarization (CPP) and electrochemical impedance spectroscopy (EIS) were performed. Scanning electron microscopy (SEM) observations were made following the CPP tests. The Zr5Ti alloy was the most susceptible to localized corrosion. The Zr25Ti alloy presents a dangerous breakdown potential but have a sufficiently negative zero corrosion potential that the difference between them is sufficiently to provide a higher localized corrosion resistance in comparison with Zr5Ti. Among ZrTi alloys subjected to investigation, the Zr45Ti alloy had a much larger passive range in the polarization curve and was the most resistant to localized corrosion. For used test conditions, the localized corrosion was not found for the cp-Ti. The EIS tests show that both investigated ZrTi alloys and cp-Ti exhibit passivity after 168h immersion in 0.9% NaCl solution, at open circuit potential.
引用
收藏
页码:585 / 591
页数:7
相关论文
共 41 条
[1]   EIS study of porous NiTi biomedical alloy in simulated body fluid [J].
Attarchi, M. ;
Mazloumi, M. ;
Behckam, I. ;
Sadrnezhaad, S. K. .
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2009, 60 (11) :871-875
[2]   Corrosion aspects of metallic implants - An overview [J].
Balamurugan, A. ;
Rajeswari, S. ;
Balossier, G. ;
Rebelo, A. H. S. ;
Ferreira, J. M. F. .
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2008, 59 (11) :855-869
[3]   Electrochemical behaviour and surface characterisation of Zr exposed to an SBF solution containing glycine, in view of dental implant applications [J].
Bozzini, Benedetto ;
Carlino, Paolo ;
Mele, Claudio .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2011, 22 (01) :193-200
[4]   Electrochemical studies on the stability and corrosion resistance of new zirconium-based alloys for biomedical applications [J].
Branzoi, Loan Viorel ;
Iordoc, Mihai ;
Codescu, Mirela .
SURFACE AND INTERFACE ANALYSIS, 2008, 40 (3-4) :167-173
[5]  
Bundy K.J., 1995, CORROSION TESTS STAN, P411
[6]   INVESTIGATION OF PASSIVE LAYERS ON IRON AND IRON-CHROMIUM ALLOYS BY ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY [J].
CASTRO, EB ;
VILCHE, JR .
ELECTROCHIMICA ACTA, 1993, 38 (11) :1567-1572
[7]   THE ANODIC BEHAVIOR OF NIOBIUM .2. GENERAL EXPERIMENTAL ELECTROCHEMICAL ASPECTS [J].
DALKAINE, CV ;
DESOUZA, LMM ;
NART, FC .
CORROSION SCIENCE, 1993, 34 (01) :117-127
[8]   Evaluation of localized corrosion of zirconium in acidic chloride solutions [J].
Fahey, J ;
Holmes, D ;
Yau, TL .
CORROSION, 1997, 53 (01) :54-61
[9]  
Frankel G.S., 2003, ASM HDB A, V13A
[10]   COMBINED ELECTROCHEMICAL AND SURFACE ANALYTICAL INVESTIGATIONS OF THE FORMATION OF PASSIVE LAYERS [J].
HAUPT, S ;
STREHBLOW, HH .
CORROSION SCIENCE, 1989, 29 (2-3) :163-182