Arc corrosion behavior of Cu-Ti3AlC2 composites in air atmosphere

被引:16
作者
Huang, XiaoChen [1 ]
Feng, Yi [1 ,2 ]
Qian, Gang [2 ]
Zhao, Hao [1 ]
Song, ZhaoKun [1 ]
Zhang, JingCheng [2 ]
Zhang, XueBin [1 ]
机构
[1] Hefei Univ Technol, rch Mat Sci & Engn, Hefei 230009, Anhui, Peoples R China
[2] Hefei Univ Technol, Instrumental Anal Ctr, Hefei 230009, Anhui, Peoples R China
基金
中国国家自然科学基金;
关键词
Cu-Ti3AlC2; arc erosion; FE-SEM; Raman spectroscopy; ELECTRON-IRRADIATION; M(N+1)AX(N) PHASES; CATHODE SPOT; MAX PHASES; VACUUM-ARC; EROSION; PROGRESS;
D O I
10.1007/s11431-017-9166-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The arc corrosion evolution of Cu-20 vol.% Ti3AlC2 cathodes is presented here. After eroded by 3, 4, 5, 6, 7, 8, 9, 10 kV DC voltage, respectively, the surface morphologies were characterized by field emission scanning electron microscope with craters and protrusions. Compared to small craters and dense protrusions of the morphology by high voltage, the eroded surface was covered with bigger craters and sparse protrusions at low voltage. No crack was discovered on the surface even at 10 kV. By means of energy dispersive spectroscopy and Raman spectroscopy, the decomposition of Cu-20 vol.% Ti3AlC2 cathode to CuO, Al2O3 and TiO2 were proved. Meanwhile, W anode is oxidized to WO2. The peak current increases with the increasing breakdown voltage, which is recorded by a digital memory oscilloscope.
引用
收藏
页码:551 / 557
页数:7
相关论文
共 27 条
  • [1] Chopping effect observed at cathodic arc initiation
    Anders, A
    [J]. IEEE TRANSACTIONS ON PLASMA SCIENCE, 2000, 28 (04) : 1303 - 1304
  • [2] The MN+1AXN phases:: A new class of solids;: Thermodynamically stable nanolaminates
    Barsoum, MW
    [J]. PROGRESS IN SOLID STATE CHEMISTRY, 2000, 28 (1-4) : 201 - 281
  • [3] Twenty-five years of progress in vacuum arc research and utilization
    Boxman, RL
    Goldsmith, S
    Greenwood, A
    [J]. IEEE TRANSACTIONS ON PLASMA SCIENCE, 1997, 25 (06) : 1174 - 1186
  • [4] The Mn+1AXn phases: Materials science and thin-film processing
    Eklund, Per
    Beckers, Manfred
    Jansson, Ulf
    Hogberg, Hans
    Hultman, Lars
    [J]. THIN SOLID FILMS, 2010, 518 (08) : 1851 - 1878
  • [5] Effect of pulsed gas tungsten arc welding process parameters on pitting corrosion resistance of type 304L stainless steel welds
    Giridharan, P. K.
    Murugan, N.
    [J]. CORROSION, 2007, 63 (05) : 433 - 441
  • [6] Formation of two-dimensional periodic microstructures by a single shot of three interfered femtosecond laser pulses on the surface of silica glass
    Guo, Zhongyi
    Qu, Shiliang
    Ran, Lingling
    Han, Yanhua
    Liu, Shutian
    [J]. OPTICS LETTERS, 2008, 33 (20) : 2383 - 2385
  • [7] Cathode spot initiation in different external conditions
    He, ZJ
    Haug, R
    [J]. JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1997, 30 (04) : 603 - 613
  • [8] Influence of breakdown voltages on arc erosion of a Ti3AlC2 cathode in an air atmosphere
    Huang, Xiaochen
    Feng, Yi
    Qian, Gang
    Zhang, Jingcheng
    Zhang, Xuebin
    [J]. CERAMICS INTERNATIONAL, 2017, 43 (13) : 10601 - 10605
  • [9] Effect of electron irradiation on different crystal planes of titanium aluminum carbide
    Huang, Xiaochen
    Feng, Yi
    Qian, Gang
    Wang, Yang
    Zhang, Xuebin
    [J]. CERAMICS INTERNATIONAL, 2016, 42 (13) : 14984 - 14991
  • [10] Effect of electron irradiation on Ti3AlC2
    Huang, Xiaochen
    Feng, Yi
    Dou, Yakun
    Tang, Hai
    Ding, Dongdong
    Tian, Pei
    Xia, Meng
    Qian, Gang
    Wang, Yang
    Zhang, Xuebin
    [J]. SCRIPTA MATERIALIA, 2016, 113 : 114 - 117