摘要
Statement of problem. Mechanical properties of denture acryl I c resins are important for the clinical success of multiple types of prostheses. Acrylic resins must be strong and resilient so as to withstand Impact. Few studies utilize cyclic loads to characterize material response to repeated stress. Purpose. The purpose of this study was to evaluate static and dynamic flexure properties of a variety of acrylic resins utilized in the fabrication of prostheses: (11) heat-polymerized polymethyl methacrylate (PMMA), powder-liquid type, and (2) a newly introduced, visible light-polymerized urethane dimethacrylate dough type. Material and methods. Twenty rectangular bars each of 4 PMMA acrylic resin materials (Diamond D, Fricke HI-1, Lucitone 199, Nature-Cryl Hi-Plus) and 1 urethane dimethacrylate (Eclipse) were fabricated and stored in 100% humidity for 30 days. Half of the specimens for each group were submitted to a static 3-point flexure test. The other half was submitted to cycling loading at 5 Hz for 10(4) cycles. Data were analyzed using 1-way ANOVA and 2-way ANOVA, followed by Tukey HSD or Bonferroni post hoc tests when necessary (alpha=.05). Results. Mean static flexure strength (SDs) in MPa were: Eclipse, 127.11 (5.83); Diamond D, 84.92 (5.10); Lucitone 199, 83.96 (11.96); HI-1, 79.54 (5.84); and Nature-Cryl Hi-Plus, 75.82 (6.96). Mean flexural strengths (SDs) in MPa postcycling were: Eclipse, 113.36 (31.29); Diamond D, 88.26 (5.46); Nature-Cryl Hi-Plus, 81.86 (4.93); HI-1, 79.18 (6.60); and Lucitone 199, 74.34 (4.95). Conclusions. The visible light-polymerized urethane dimethacrylate resin (Eclipse) showed greater flexure strength than all PMMA heat-polymerized resins for both static and cycled groups (P <.001). Yet the Eclipse material had lower load limits, and demonstrated brittle-type behavior and greater standard deviations. The heat-polymerized PMMA materials did not significantly differ from each other after static or cyclic testing.
引用
收藏
页码:47 / 51
页数:5
相关论文
共 17 条
  • [1] EFFECT OF WATER AND ARTIFICIAL SALIVA ON MECHANICAL-PROPERTIES OF SOME DENTURE-BASE MATERIALS
    ALMULLA, MAS
    MURPHY, WM
    HUGGETT, R
    BROOKS, SC
    [J]. DENTAL MATERIALS, 1989, 5 (06) : 399 - 402
  • [2] COLLINS JA, 1993, ANAL PREDICTION PREV, P383
  • [3] Effect of relining, water storage and cyclic loading on the flexural strength of a denture base acrylic resin
    dos Santos Nunes Reis, Jose Mauricio
    Eduardo Vergani, Carlos
    Claudia Pavarina, Ana
    Teresinha Giampaolo, Eunice
    Lucia Machado, Ana
    [J]. JOURNAL OF DENTISTRY, 2006, 34 (07) : 420 - 426
  • [4] Fujii K, 1989, Dent Mater J, V8, P243
  • [5] *INT STAND ORG, 1999, 1567 ISO
  • [6] An investigation into the transverse and impact strength of 'high strength' denture base acrylic resins
    Jagger, DC
    Jagger, RG
    Allen, SM
    Harrison, A
    [J]. JOURNAL OF ORAL REHABILITATION, 2002, 29 (03) : 263 - 267
  • [7] Flexural strength of heat-polymerized polymethyl methacrylate denture resin reinforced with glass, aramid, or nylon fibers
    John, J
    Gangadhar, SA
    Shah, I
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2001, 86 (04) : 424 - 427
  • [8] FLEXURE FATIGUE OF 10 COMMONLY USED DENTURE BASE RESINS
    JOHNSTON, EP
    NICHOLLS, JI
    SMITH, DE
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1981, 46 (05) : 478 - 483
  • [9] FATIGUE FAILURE IN DENTURE BASE POLYMERS
    KELLY, E
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1969, 21 (03) : 257 - &
  • [10] THE STAINING CHARACTERISTICS, TRANSVERSE STRENGTH, AND MICROHARDNESS OF A VISIBLE LIGHT-CURED DENTURE BASE MATERIAL
    KHAN, Z
    VONFRAUNHOFER, JA
    RAZAVI, R
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1987, 57 (03) : 384 - 386