Iron-containing intermetallic phases in Al-Si based casting alloys

被引:313
作者
Taylor, John A. [1 ]
机构
[1] Univ Queensland, CAST Cooperat Res Ctr CAST CRC, Sch Mech & Min Engn, Brisbane, Qld 4072, Australia
来源
11TH INTERNATIONAL CONGRESS ON METALLURGY & MATERIALS SAM/CONAMET 2011 | 2012年 / 1卷
关键词
Al-Si alloys; intermetallics; castability; mechanical properties; ALUMINUM; POROSITY; MICROSTRUCTURE; PARTICLES; DUCTILITY; BEHAVIOR; SILICON;
D O I
10.1016/j.mspro.2012.06.004
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Iron is the most common impurity in aluminium and its alloys. It is not easily removed and it can cause adverse effects to ductility and castability, particularly in the popular Al-Si based casting alloys. The choice of whether to use alloys based on primary aluminium (low Fe levels, high cost) or secondary aluminium (moderate/high Fe levels, cheaper) for a cast product is often a commercial decision. However, a compromise may be necessary between the desire for reduced metal cost and the need to maximise casting productivity via reduced defect formation and to minimise the deleterious effect of iron on mechanical properties. This paper discusses the various sources of iron, how it enters aluminium alloys, the way that iron leads to the formation of complex intermetallic phases during solidification and how these phases can adversely affect mechanical properties (especially ductility) and lead to the formation of excessive shrinkage defects. The formation of the iron-containing beta phase will be highlighted using the latest in situ solidification study using synchrotron X-radiation. The paper offers guidelines to the practical levels of iron that can be tolerated and how to minimise the negative effects of iron. (C) 2012 Published by Elsevier Ltd. Selection and/or peer-review under responsibility of SAM/CONAMET 2011, Rosario, Argentina.
引用
收藏
页码:19 / 33
页数:15
相关论文
共 39 条
[1]  
[Anonymous], T AM FOUNDRYMANS SOC
[2]  
Apelian D., 1990, AFS T, V97, P727
[3]   Enhanced ductility in Al-Si-Cu-Mg foundry alloys with high Si content [J].
Caceres, C. H. ;
Taylor, J. A. .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2006, 37 (06) :897-903
[4]   Strength-ductility behaviour of Al-Si-Cu-Mg casting alloys in T6 temper [J].
Cáceres, CH ;
Svensson, IL ;
Taylor, JA .
INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2003, 15 (05) :531-543
[5]  
Chen XG, 1998, LIGHT METALS 1998, P1071
[6]  
COUTURE A, 1981, INT CAST MET J, V6, P9
[7]  
Dinnis C.M., 2007, 5th decennial conference on solidification processing, P566
[8]   Iron-related porosity in Al-Si-(Cu) foundry alloys [J].
Dinnis, Cameron M. ;
Taylor, John A. ;
Dahle, Arne K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 425 (1-2) :286-296
[9]   As-cast morphology of iron-intermetallics in Al-Si foundry alloys [J].
Dinnis, CM ;
Taylor, JA ;
Dahle, AK .
SCRIPTA MATERIALIA, 2005, 53 (08) :955-958
[10]  
Dinnis CM, 2004, P 9 INT C AI ALL, P1016