Synergistic thermal stabilization of ceramic/co-polyimide coated polypropylene separators for lithium-ion batteries
被引:118
作者:
Lee, Yunju
[1
]
Lee, Hoogil
[1
]
Lee, Taejoo
[1
]
Ryou, Myung-Hyun
[1
]
Lee, Yong Min
[1
]
机构:
[1] Hanbat Natl Univ, Dept Chem & Biol Engn, Taejon 305719, South Korea
基金:
新加坡国家研究基金会;
关键词:
Polyimide;
Polypropylene;
Separators;
Thermal shrinkage;
Lithium-ion batteries;
POLYETHYLENE SEPARATORS;
COMPOSITE SEPARATORS;
PERFORMANCE;
DEPOSITION;
STABILITY;
D O I:
10.1016/j.jpowsour.2015.06.106
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
To improve the safety of lithium-ion batteries (LIBs), co-polyimide (PI) P84 was introduced as a polymeric binder for Al2O3/Polymer composite surface coatings on polypropylene (PP) separators. By monitoring the dimensional shrinkage of the PP separators at high temperatures, we verified a synergistic thermal stabilization effect between the Al2O3 ceramic and the PI polymeric binder. Although PI was thermally stable up to 300 degrees C, a coating consisting solely of PI did not impede the PP separator dimensional changes (-22% at 150 degrees C). On the other hand, the Al2O3/PI-coated PP separators efficiently impeded the thermal shrinkage (-10% at 150 degrees C). In contrast, an Al2O3/poly(vinylidene fluoride-co-hexafluoropropylene) (PVdF-HFP) combination lowered the thermal stability of the PP separators (-33% at 150 degrees C). As a result, the Al2O3/PI-coated PP separators remarkably suppressed the internal short-circuit of the unit half-cells associated with separator thermal shrinkage (100 min at 160 degrees C), whereas the PVdF-HFP retained only 40 min under identical conditions. The Al2O3/PI-coated PP separators achieved rate capabilities and cell performances similar to those of the bare PP separators. (C) 2015 Elsevier B.V. All rights reserved.