Scrubbing Effect of Self-etching Adhesives on Bond Strength to NaOCl-treated Dentin

被引:16
作者
Prasansuttiporn, Taweesak [1 ,2 ]
Nakajima, Masatoshi
Foxton, Richard M. [3 ,4 ,5 ]
Tagami, Junji [2 ]
机构
[1] Tokyo Med & Dent Univ, Dept Restorat Sci, Grad Sch, Bunkyo Ku, Tokyo 1138549, Japan
[2] Tokyo Med & Dent Univ, Int Res Ctr Mol Sci Tooth & Bone Dis, Global Ctr Excellence GCOE Program, Tokyo 1138549, Japan
[3] Kings Coll London, Inst Dent, Div Conservat Dent, Guys Hosp, London WC2R 2LS, England
[4] Kings Coll London, Inst Dent, Div Conservat Dent, Kings Hosp, London WC2R 2LS, England
[5] Kings Coll London, Inst Dent, Div Conservat Dent, St Thomas Hosp, London WC2R 2LS, England
关键词
sodium hypochlorite; scrubbing; dentin; bond strength; adhesives; SODIUM-HYPOCHLORITE TREATMENT; PRIMER; ENAMEL;
D O I
10.3290/j.jad.a22340
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the scrubbing effect of self-etching adhesive systems on the microtensile bond strengths to sodium hypochlorite-treated dentin. Materials and Methods: The occlusal surfaces of 36 extracted human third molars were horizontally cut to expose sound dentin. The dentin surfaces of the teeth were treated with 6% NaOCl aqueous solution for 30 s or none. After water rinsing for 10 s and air drying, a 2-step (Clearfil Protect Bond) or 1-step (Clearfil S-3 Bond or Bond Force) self-etching adhesive was applied with or without a scrubbing technique, and resin composite (Clearfil AP-X) crowns were built up. The bonded specimens were stored in water for 24 h and then subjected to the microtensile bond test at a crosshead speed of 1.0 mm/min. Data were analyzed using three-way ANOVA and Bonferroni multiple comparisons (p < 0.05). Results: The NaOCl-treated dentin exhibited significantly lower bond strength with the tested self-etching adhesive systems than did the normal dentin (p < 0.05). Using a scrubbing technique for the tested self-etching adhesive systems significantly improved the mu TBS to NaOCl-treated dentin (p < 0.05), whereas there was no significant difference in mu TBS to normal dentin between a scrubbing and nonscrubbing technique (p > 0.05). Conclusion: Using a scrubbing technique for applying self-etching adhesive systems to NaOCl-treated dentin was effective in improving the compromised bonding.
引用
收藏
页码:121 / 127
页数:7
相关论文
共 23 条
[1]  
Bowen R L, 1984, Oper Dent Suppl, V3, P30
[2]  
Chan KM, 2003, AM J DENT, V16, P340
[3]   Effect of medications for root canal treatment on bonding to root canal dentin [J].
Erdemir, A ;
Ari, H ;
Güngünes, H ;
Belli, S .
JOURNAL OF ENDODONTICS, 2004, 30 (02) :113-116
[4]  
Gokce K, 2008, J ADHES DENT, V10, P345
[5]   INTERACTION BETWEEN THE DENTINAL SMEAR LAYER AND COMPOSITE BOND STRENGTH [J].
ISHIOKA, S ;
CAPUTO, AA .
JOURNAL OF PROSTHETIC DENTISTRY, 1989, 61 (02) :180-185
[6]  
Jain M., 2009, TXB ENG PHYS 1, P1
[7]   Effect of dentin pretreatment with mild acidic HOCl solution on microtensile bond strength and surface pH [J].
Kunawarote, Sitthikorn ;
Nakajima, Masatoshi ;
Shida, Kanako ;
Kitasako, Yuichi ;
Foxton, Richard M. ;
Tagami, Junji .
JOURNAL OF DENTISTRY, 2010, 38 (03) :261-268
[8]   Reversal of compromised bonding to oxidized etched dentin [J].
Lai, SCN ;
Mak, YF ;
Cheung, GSP ;
Osorio, R ;
Toledano, M ;
Carvalho, RM ;
Tay, FR ;
Pashley, DH .
JOURNAL OF DENTAL RESEARCH, 2001, 80 (10) :1919-1924
[9]  
Miyazaki M, 2002, AM J DENT, V15, P412
[10]  
Montes MAJR, 2005, OPER DENT, V30, P201