Three-dimensional investigation of the texture and microstructure below a nanoindent in a Cu single crystal using 3D EBSD and crystal plasticity finite element simulations

被引:262
作者
Zaafarani, N
Raabe, D
Singh, RN
Roters, F
Zaefferer, S
机构
[1] Max Planck Inst Eisenforsch GmbH, Abt Mikrostruckturphys & Umformtech, D-40237 Dusseldorf, Germany
[2] Bhabha Atom Res Ctr, Div Sci Mat, Mech Met Sect, Bombay 400085, Maharashtra, India
关键词
3D EBSD; focused ion beam; texture; nanoindentation; copper;
D O I
10.1016/j.actamat.2005.12.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper reports a three-dimensional (3D) study of the microstructure and texture below a conical nanoindent in a (1 1 1) CU single crystal at nanometer-scale resolution. The experiments are conducted using a joint high-resolution field emission scanning electron microscopy/electron backscatter diffraction (EBSD) Set-Lip Coupled with serial sectioning in a focused ion beam system in the form of a cross-beam 3D crystal orientation microscope (3D EBSD). The experiments (conducted in sets of subsequent (1 1 2) cross-section planes) reveal a pronounced deformation-induced 3D patterning of the lattice rotations below the indent. In the cross-section planes perpendicular to the (1 1 1) surface plane below the indenter tip the observed deformation-induced rotation pattern is characterized by an outer tangent zone with large absolute values of the rotations and an inner zone closer to the indenter axis with small rotations. The mapping of the rotation directions reveals multiple transition regimes with steep orientation gradients and frequent changes in sign. The experiments are compared to 3D elastic-viscoplastic crystal plasticity finite element Simulations adopting the geometry and boundary conditions of the experiments. The Simulations show a similar pattern for the absolute orientation changes but they fail to predict the fine details of the patterning of the rotation directions with the frequent changes in sign observed in the experiment. Also the simulations overemphasize the magnitude of the rotation field tangent to the indenter relative to that directly below the indenter tip. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1863 / 1876
页数:14
相关论文
共 47 条
[1]   On the evolution of crystallographic dislocation density in non-homogeneously deforming crystals [J].
Arsenlis, A ;
Parks, DM ;
Becker, R ;
Bulatov, VV .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2004, 52 (06) :1213-1246
[2]   White microbeam diffraction from distorted crystals [J].
Barabash, R ;
Ice, GE ;
Larson, BC ;
Pharr, GM ;
Chung, KS ;
Yang, W .
APPLIED PHYSICS LETTERS, 2001, 79 (06) :749-751
[3]   Influences of pileup on the measurement of mechanical properties by load and depth sensing indentation techniques [J].
Bolshakov, A ;
Pharr, GM .
JOURNAL OF MATERIALS RESEARCH, 1998, 13 (04) :1049-1058
[4]   Size effects on the onset of plastic deformation during nanoindentation of thin films and patterned lines [J].
Choi, Y ;
Van Vliet, KJ ;
Li, J ;
Suresh, S .
JOURNAL OF APPLIED PHYSICS, 2003, 94 (09) :6050-6058
[5]   Indentation size effect in metallic materials:: Correcting for the size of the plastic zone [J].
Durst, K ;
Backes, B ;
Göken, M .
SCRIPTA MATERIALIA, 2005, 52 (11) :1093-1097
[6]   Finite element study for nanoindentation measurements on two-phase materials [J].
Karsten Durst ;
Mathias Göken ;
Horst Vehoff .
Journal of Materials Research, 2004, 19 (1) :85-93
[7]   Finite element simulation of spherical indentation in the elastic-plastic transition [J].
Durst, K ;
Göken, M ;
Pharr, GM .
ZEITSCHRIFT FUR METALLKUNDE, 2002, 93 (09) :857-861
[8]   Non-local crystal plasticity model with intrinsic SSD and GND effects [J].
Evers, LP ;
Brekelmans, WAM ;
Geers, MGD .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2004, 52 (10) :2379-2401
[9]   Crystal plasticity model with enhanced hardening by geometrically necessary dislocation accumulation [J].
Evers, LP ;
Parks, DM ;
Brekelmans, WAM ;
Geers, MGD .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2002, 50 (11) :2403-2424
[10]  
FISCHERCRIPPS AC, 2004, SPRINGER MECH ENG SE