Corrosion Initiation and Propagation on Carburized Martensitic Stainless Steel Surfaces Studied via Advanced Scanning Probe Microscopy

被引:14
作者
Kvryan, Armen [1 ]
Efaw, Corey M. [1 ]
Higginbotham, Kari A. [1 ]
Maryon, Olivia O. [1 ]
Davis, Paul H. [1 ]
Graugnard, Elton [1 ]
Trivedi, Hitesh K. [2 ]
Hurley, Michael F. [1 ]
机构
[1] Boise State Univ, Micron Sch Mat Sci & Engn, Boise, ID 83725 USA
[2] UES Inc, 4401 Dayton Xenia Rd, Dayton, OH 45432 USA
基金
美国国家科学基金会;
关键词
corrosion; bearing steels; martensitic stainless steel; aerospace; atomic force microscopy (AFM); scanning Kelvin probe microscopy (SKPFM); nanoscale; electrochemistry; wear; Pyrowear; 675; AMS; 5930; MAGNETIC FORCE MICROSCOPY; POTENTIAL MEASUREMENTS; LOCALIZED CORROSION; BEARING STEELS; MICROSTRUCTURE; BEHAVIOR; SKPFM; AFM; TEMPERATURE; AA2024-T3;
D O I
10.3390/ma12060940
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Historically, high carbon steels have been used in mechanical applications because their high surface hardness contributes to excellent wear performance. However, in aggressive environments, current bearing steels exhibit insufficient corrosion resistance. Martensitic stainless steels are attractive for bearing applications due to their high corrosion resistance and ability to be surface hardened via carburizing heat treatments. Here three different carburizing heat treatments were applied to UNS S42670: a high-temperature temper (HTT), a low-temperature temper (LTT), and carbo-nitriding (CN). Magnetic force microscopy showed differences in magnetic domains between the matrix and carbides, while scanning Kelvin probe force microscopy (SKPFM) revealed a 90-200 mV Volta potential difference between the two phases. Corrosion progression was monitored on the nanoscale via SKPFM and in situ atomic force microscopy (AFM), revealing different corrosion modes among heat treatments that predicted bulk corrosion behavior in electrochemical testing. HTT outperforms LTT and CN in wear testing and thus is recommended for non-corrosive aerospace applications, whereas CN is recommended for corrosion-prone applications as it exhibits exceptional corrosion resistance. The results reported here support the use of scanning probe microscopy for predicting bulk corrosion behavior by measuring nanoscale surface differences in properties between carbides and the surrounding matrix.
引用
收藏
页数:20
相关论文
共 63 条
[51]  
Schneider M.J., 2013, Steel Heat Treating Fundamentals and Processes, P389, DOI [10.31399/asm.hb.v04a.a0005771, DOI 10.31399/ASM.HB.V04A.A0005771]
[52]  
Smallman RE, 2007, PHYSICAL METALLURGY AND ADVANCED MATERIALS, 7TH EDITION, P1
[53]   Magnetic properties of the UNS S39205 duplex stainless steel [J].
Tavares, SSM ;
Pedrosa, PDS ;
Teodósio, JR ;
da Silva, MR ;
Neto, JM ;
Pairis, S .
JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 351 (1-2) :283-288
[54]   Magnetic property changes during embrittlement of a duplex stainless steel [J].
Tavares, SSM ;
da Silva, MR ;
Neto, JM .
JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 313 :168-173
[55]   Residual stress and microstructure in welds of 13%Cr-4%Ni martensitic stainless steel [J].
Thibault, Denis ;
Bocher, Philippe ;
Thomas, Marc .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (04) :2195-2202
[56]  
Trivedi H., 2017, ASTM STP, P275
[57]   Low Temperature Plasma Nitriding of Pyrowear 675 [J].
Trivedi, Hitesh K. ;
Monahan, Ray .
BEARING STEEL TECHNOLOGIES: 10TH VOLUME: ADVANCES IN STEEL TECHNOLOGIES FOR ROLLING BEARINGS, 2015, 1580 :444-464
[58]   Effect of Silicon Nitride Ball on Adhesive Wear of Martensitic Stainless Steel Pyrowear 675 and AISI M-50 Races with Type II Ester Oil [J].
Trivedi, Hitesh K. ;
Wedeven, Vern ;
Black, William .
TRIBOLOGY TRANSACTIONS, 2016, 59 (02) :363-374
[59]  
WERT DE, 1994, ADV MATER PROCESS, V145, P89
[60]   Rolling bearing steels - a technical and historical perspective [J].
Zaretsky, E. V. .
MATERIALS SCIENCE AND TECHNOLOGY, 2012, 28 (01) :58-69