Photoluminescence properties of KSrPO4:Sm3+ phosphor for SSL applications

被引:9
作者
Bora, R. G. [1 ]
Palan, C. B. [2 ]
Sawala, N. S. [3 ]
Korpe, G. V. [4 ]
Omanwar, S. K. [1 ]
机构
[1] St Gadge Baba Amravati Univ, Dept Phys, Amravati 444602, India
[2] Dept ASH MGI COET, Shegaon 444203, India
[3] Govt Polytech, Arvi 442201, India
[4] Shri Shivaji Coll Arts Commerce & Sci, Akola 444001, India
关键词
LIGHT-EMITTING-DIODES; LUMINESCENCE PROPERTIES; RADIATION-DOSIMETRY; SM PHOSPHORS; MICROSTRUCTURE; TEMPERATURE; GLASSES; FLUX; TB; EU;
D O I
10.1007/s10854-017-7945-8
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The orange light emitting KSr(1-x)PO4:xSm3+ (x = 0.001, 0.002, 0.005, 0.01 and 0.02) phosphors were successfully synthesized via solid-state diffusion method. The phase of the prepared KSrPO4:Sm3+ phosphor was confirmed by powder XRD analysis and studied its photoluminescence (PL) properties under ultraviolet (UV) excitation (300-450 nm). The XRD pattern of prepared KSrPO4:Sm3+ phosphor is well matched with available standard ICDD file having card no. 00-033-1045. The excitation and emission spectra of prepared phosphor were monitored at 598 and 402 nm respectively. The PL emission spectra of prepared KSrPO4:Sm phosphor consists of series of sharp lines peak at 559, 598, and 644 nm, to the corresponding to (4)G(5/2) -> H-6(5/2), (4)G(5/2) -> H-6(7/2) and (4)G(5/2) -> H-6(9/2) transitions of Sm3+ ion respectively. The optimum PL intensity is obtained at 0.005 mol of Sm3+ ion at 402 nm excitation. The CIE (Commission International de l'Eclairage) coordinates of prepared phosphor was calculated and found to x = 0.6177, y = 0.3817. Hence the KSrPO4:Sm has great potential in solid state lighting and light-emitting diode applications.
引用
收藏
页码:541 / 545
页数:5
相关论文
共 28 条
[1]   Optical spectroscopy and waveguide fabrication in Sm3+/Tb3+ doped zinc-sodium-aluminosilicate glasses [J].
Caldino, U. ;
Speghini, A. ;
Berneschi, S. ;
Bettinelli, M. ;
Brenci, M. ;
Pelli, S. ;
Righini, G. C. .
OPTICAL MATERIALS, 2012, 34 (07) :1067-1071
[2]   ROOM-TEMPERATURE PERSISTENT HOLE-BURNING OF SM2+ IN OXIDE GLASSES [J].
HIRAO, K ;
TODOROKI, S ;
CHO, DH ;
SOGA, N .
OPTICS LETTERS, 1993, 18 (19) :1586-1587
[3]  
Hu X.F., 2009, POWDER TECHNOL, V188, P242
[4]  
Jing Q., 2013, J APPL PHYS, V113
[5]   Full-color and thermally stable KSrPO4:Ln (Ln = Eu, Tb, Sm) phosphors for white-light-emitting diodes [J].
Lin, C. C. ;
Liu, R. S. ;
Tang, Y. S. ;
Hu, S. F. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2008, 155 (09) :J248-J251
[6]   KBaPO4:Ln (Ln = Eu, Tb, Sm) phosphors for UV excitable white light-emitting diodes [J].
Lin, C. C. ;
Tang, Y. S. ;
Hu, S. F. ;
Liu, R. S. .
JOURNAL OF LUMINESCENCE, 2009, 129 (12) :1682-1684
[7]   Versatile Phosphate Phosphors ABPO4 in White Light-Emitting Diodes: Collocated Characteristic Analysis and Theoretical Calculations [J].
Lin, Chun Che ;
Xiao, Zhi Ren ;
Guo, Guang-Yu ;
Chan, Ting-Shan ;
Liu, Ru-Shi .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2010, 132 (09) :3020-3028
[8]   Photoluminescence properties of Eu3+/ Sm3+ activated CaZr4(PO4)6 phosphors [J].
Nair, Govind B. ;
Dhoble, S. J. .
JOURNAL OF FLUORESCENCE, 2016, 26 (05) :1865-1873
[9]   Spatially resolved measurement of high doses in microbeam radiation therapy using samarium doped fluorophosphate glasses [J].
Okada, Go ;
Morrell, Brian ;
Koughia, Cyril ;
Edgar, Andy ;
Varoy, Chris ;
Belev, George ;
Wysokinski, Tomasz ;
Chapman, Dean ;
Kasap, Safa .
APPLIED PHYSICS LETTERS, 2011, 99 (12)
[10]   Synthesis and preliminary OSL studies of NaCaPO4:Ce phosphor for radiation dosimetry [J].
Palan, C. B. ;
Omanwar, S. K. .
RESEARCH ON CHEMICAL INTERMEDIATES, 2017, 43 (07) :4043-4050