Reliability enhancement of Sn-1.0Ag-0.5Cu nano-composite solders by adding multiple sizes of TiO2 nanoparticles

被引:45
|
作者
Wen, Yanni [1 ]
Zhao, Xiuchen [1 ]
Chen, Zhuo [1 ]
Gu, Yue [2 ]
Wang, Yong [1 ]
Chen, Zhiwei [1 ]
Wang, Xinyuan [1 ]
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, 5 Yard,Zhong Guan Cun South St, Beijing 100081, Peoples R China
[2] Univ Calif San Diego, Dept Nanoengn, Mat Sci & Engn Program, La Jolla, CA 92093 USA
关键词
TiO2 nanoparticles size; SAC105; solder; Thermal cycling; Joint reliability; AG-CU SOLDER; INTERFACIAL INTERMETALLIC GROWTH; MECHANICAL-PROPERTIES; MICROSTRUCTURE; WETTABILITY; PARTICLES; ADDITIONS; JOINTS; HARDNESS; PASTES;
D O I
10.1016/j.jallcom.2016.12.037
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper demonstrates a novel low silver content TiO2 nanoparticle composite solder alloys, and discusses the TiO2 size effect on reliability of the solder and its solder joints with copper. 6 nm and 20 nm TiO2 nanoparticles were synthesized and added into Sn-1.0Ag-0.5Cu (SAC105) solder to prepare the nano-composite solders. The microstructure, coefficient of thermal expansion of the solders, and the shear strength, interfacial intermetallic compound growth of the solder joints under thermal cycling (1000 cycles) between -55 degrees C and 125 degrees C were investigated. The experimental results show that TiO2 nanoparticles can refine beta-Sn grain size, decrease CTE of the solders, as well as suppress the interfacial intermetallic compound formation and growth. Also, after thermal cycling, the nano-composite solder joints have higher shear strength than the joints without TiO2 nanoparticles. Most importantly, smaller TiO2 nanoparticles (6 nm) shows larger influence on the respects of microstructure refinement, coefficient of thermal expansion reduction, interfacial IMC thickness decrease, and shear strength enhancement of the solder joints. The TiO2 nano-composite solder joints show higher electrical reliability than the original SAC105 solder joint according to the results of electric resistance change during thermal cycling. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:799 / 807
页数:9
相关论文
共 50 条
  • [1] Effect of TiO2 addition concentration on the wettability and intermetallic compounds growth of Sn3.0Ag0.5Cu-xTiO2 nano-composite solders
    Li, Yi
    Zhao, XiuChen
    Liu, Ying
    Wang, Yuan
    Wang, Yong
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2014, 25 (09) : 3816 - 3827
  • [2] Effect of TiO2 addition concentration on the wettability and intermetallic compounds growth of Sn3.0Ag0.5Cu–xTiO2 nano-composite solders
    Yi Li
    XiuChen Zhao
    Ying Liu
    Yuan Wang
    Yong Wang
    Journal of Materials Science: Materials in Electronics, 2014, 25 : 3816 - 3827
  • [3] Properties of (Fe-B)-doped Sn-1.0Ag-0.5Cu solders prepared by mechanical alloying
    Wang, Ruo-Da
    Hu, Qiang
    Zhang, Shao-Ming
    Zhang, Fu-Wen
    Lu, Cai-Tao
    Wang, Zhi-Gang
    RARE METALS, 2019, 38 (07) : 665 - 674
  • [4] Effect of γ-Fe2O3 nanoparticles size on the properties of Sn-1.0Age0.5Cu nano-composite solders and joints
    Zhao, Xiuchen
    Wen, Yanni
    Li, Yi
    Liu, Ying
    Wang, Yong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 662 : 272 - 282
  • [5] Properties of (Fe-B)-doped Sn-1.0Ag-0.5Cu solders prepared by mechanical alloying
    Ruo-Da Wang
    Qiang Hu
    Shao-Ming Zhang
    Fu-Wen Zhang
    Cai-Tao Lu
    Zhi-Gang Wang
    RareMetals, 2019, 38 (07) : 665 - 674
  • [6] Effect of TiO2 nanoparticles on the horizontal hardness properties of Sn-3.0Ag-0.5Cu-1.0TiO2 composite solder
    Nasir, Siti Shareeda Mohd
    Yahaya, Muhamad Zamri
    Erer, Ahmet Mustafa
    Illes, Balks
    Mohamad, Ahmad Azmin
    CERAMICS INTERNATIONAL, 2019, 45 (15) : 18563 - 18571
  • [7] Research on Reliability of Sn-1.0Ag-0.5Cu Low-Ag Lead-free Solder Alloy
    Hu, Yating
    An, Bing
    Chen, Rong
    Lv, Weiwen
    Wu, Yiping
    2014 15TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY (ICEPT), 2014, : 401 - 404
  • [8] Drop impact reliability of Sn-1.0Ag-0.5Cu BGA interconnects with different mounting methods
    Wang, Bo
    Li, Jiajun
    Gallagher, Anthony
    Wrezel, James
    Towashirporn, Pongpinit
    Zhao, Naiqin
    MICROELECTRONICS RELIABILITY, 2012, 52 (07) : 1475 - 1482
  • [9] The study of Sn-0.3Ag-0.7Cu and Sn-1.0Ag-0.5Cu solder joint reliability under board level drop impact
    Gu, Jian
    Lei, Yongping
    Lin, Jian
    Fu, Hanguang
    Xie, Xiaowen
    Wu, Zhongwei
    2015 16TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY, 2015,
  • [10] Effect of Cu6Sn5 nanoparticles size on the properties of Sn0.3Ag0.7Cu nano-composite solders and joints
    Min, Zhixian
    Qiu, Yu
    Hu, Xiaowu
    Wang, Haozhong
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (15) : 14726 - 14735