Review of Laser Powder Bed Fusion of Gamma-Prime-Strengthened Nickel-Based Superalloys

被引:55
作者
Adegoke, Olutayo [1 ]
Andersson, Joel [1 ]
Brodin, Hakan [2 ]
Pederson, Robert [1 ]
机构
[1] Univ West, Dept Engn Sci, SE-46186 Trollhattan, Sweden
[2] Siemens Ind Turbomachinery, S-61283 Finspang, Sweden
关键词
laser powder bed fusion; nickel-based superalloy; microstructure; defects; cracks; DUCTILITY-DIP CRACKING; MICROSTRUCTURAL CHARACTERISTICS; MECHANICAL-PROPERTIES; METALLIC COMPONENTS; THERMAL-BEHAVIOR; RESIDUAL-STRESS; MELTING PROCESS; SINGLE-CRYSTAL; WELD METALS; IN738LC;
D O I
10.3390/met10080996
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper reviews state of the art laser powder bed fusion (L-PBF) manufacturing of gamma ' nickel-based superalloys. L-PBF resembles welding; therefore, weld-cracking mechanisms, such as solidification, liquation, strain age, and ductility-dip cracking, may occur during L-PBF manufacturing. Spherical pores and lack-of-fusion voids are other defects that may occur in gamma '-strengthened nickel-based superalloys manufactured with L-PBF. There is a correlation between defect formation and the process parameters used in the L-PBF process. Prerequisites for solidification cracking include nonequilibrium solidification due to segregating elements, the presence of liquid film between cells, a wide critical temperature range, and the presence of thermal or residual stress. These prerequisites are present in L-PBF processes. The phases found in L-PBF-manufactured gamma '-strengthened superalloys closely resemble those of the equivalent cast materials, where gamma, gamma ', and gamma/gamma ' eutectic and carbides are typically present in the microstructure. Additionally, the sizes of the gamma ' particles are small in as-built L-PBF materials because of the high cooling rate. Furthermore, the creep performance of L-PBF-manufactured materials is inferior to that of cast material because of the presence of defects and the small grain size in the L-PBF materials; however, some vertically built L-PBF materials have demonstrated creep properties that are close to those of cast materials.
引用
收藏
页码:1 / 26
页数:26
相关论文
共 85 条
[1]   Additive Manufacturing and Characterization of Rene 80 Superalloy Processed Through Scanning Laser Epitaxy for Turbine Engine Hot-Section Component Repair [J].
Acharya, Ranadip ;
Bansal, Rohan ;
Gambone, Justin J. ;
Kaplan, Max A. ;
Fuchs, Gerhard E. ;
Rudawski, N. G. ;
Das, Suman .
ADVANCED ENGINEERING MATERIALS, 2015, 17 (07) :942-950
[2]  
Adegoke O, 2019, MAT SCI TECHNOLOGY, P27
[3]  
Andersson J., 2011, WELDABILITY PRECIPIT
[4]  
[Anonymous], Application of High-Performance Polyimides in Additive Manufacturing and Powder Coating-ProQuest
[5]   Additive manufacturing of Ni-based superalloys: The outstanding issues [J].
Attallah, Moataz M. ;
Jennings, Rachel ;
Wang, Xiqian ;
Carter, Luke N. .
MRS BULLETIN, 2016, 41 (10) :758-764
[6]   Additive Manufacturing of Nickel Superalloys: Opportunities for Innovation and Challenges Related to Qualification [J].
Babu, S. S. ;
Raghavan, N. ;
Raplee, J. ;
Foster, S. J. ;
Frederick, C. ;
Haines, M. ;
Dinwiddie, R. ;
Kirka, M. K. ;
Plotkowski, A. ;
Lee, Y. ;
Dehoff, R. R. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (09) :3764-3780
[7]   Characterization of the microstructure evolution in a nickel base superalloy during continuous cooling conditions [J].
Babu, SS ;
Miller, MK ;
Vitek, JM ;
David, SA .
ACTA MATERIALIA, 2001, 49 (20) :4149-4160
[8]   Epitaxial deposition of nickel-based superalloy Rene 142 through scanning laser epitaxy (SLE) [J].
Basak, Amrita ;
Acharya, Ranadip ;
Das, Suman .
ADDITIVE MANUFACTURING, 2018, 22 :665-671
[9]   Additive Manufacturing of Nickel-Base Superalloy IN100 Through Scanning Laser Epitaxy [J].
Basak, Amrita ;
Das, Suman .
JOM, 2018, 70 (01) :53-59
[10]   Microstructures and Microhardness Properties of CMSX-4A® Additively Fabricated Through Scanning Laser Epitaxy (SLE) [J].
Basak, Amrita ;
Raghu, Shashank Holenarasipura ;
Das, Suman .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (12) :5877-5884