Effect of accelerated aging on dental zirconia-based materials

被引:48
作者
De Souza, Grace M. [1 ]
Zykus, Angelica [1 ]
Ghahnavyeh, Reza R. [1 ]
Lawrence, Samantha K. [2 ]
Bahr, David F. [2 ]
机构
[1] Univ Toronto, Dept Clin Sci, Fac Dent, 124 Edward St, Toronto, ON M5G 1G6, Canada
[2] Purdue Univ, Sch Mat Engn, 701 West Stadium Ave, W Lafayette, IN 47907 USA
关键词
Flexural strength; Phase transformation; Nanoindentation; Surface topography; YTTRIA-STABILIZED ZIRCONIA; Y-TZP; MECHANICAL-PROPERTIES; STRUCTURAL STABILITY; FLEXURAL STRENGTH; FEMORAL-HEAD; GRAIN-SIZE; TEMPERATURE; CERAMICS; DEGRADATION;
D O I
10.1016/j.jmbbm.2016.08.023
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objective: To investigate the effect of aging on phase transformation and mechanical properties of yttria-tetragonal zirconia polycrystal (Y-TZP). Materials and methods: Fully-sintered Y-TZP slabs, IPS E-max ZirCAD (ZC - Ivoclar) and Z-5 ceramic (Z5- C5 Medical Werks), were artificially aged in autoclave for: 0, 30, 60 or 90 min. Flexural strength (FS), crystalline changes (X-ray diffraction analysis - XRD) and surface topography were analyzed. 0 and 90 min-aged samples were evaluated by nanoindentation to measure hardness and modulus, and results were compared using Wilcoxan Mann Whitney rank sum test (p <= 0.05). FS results were compared using two-way ANOVA and Tukey HSD (alpha=0.05). Results: Material factor had significant effect (p=0.001) on flexural strength (Z5=966.95 MPa; ZC=847.82 MPa), but aging did not. Nanoindentation showed incidence of typical load/depth curves combined with some exhibiting features compatible with cracking. When typical curves were considered, aging had no effect on the modulus and hardness, but hardness was dependent on material type. A steady increase in the in phase related to aging time was observed for ZC samples. The maximum incidence of in phase was 6.56% for Z5/60 min. Significance: Flexural strength is not affected by surface transformation in dental Y-TZP. Hydrothermal aging has an effect on m content and surface topography of different zirconia brands, but mechanical tests that can precisely characterize surface changes in aged Y-TZP are still missing. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:256 / 263
页数:8
相关论文
共 32 条
[1]   Influence of Low-Temperature Environmental Exposure on the Mechanical Properties and Structural Stability of Dental Zirconia [J].
Alghazzawi, Tariq F. ;
Lemons, Jack ;
Liu, Perng-Ru ;
Essig, Milton E. ;
Bartolucci, Alfred A. ;
Janowski, Gregg M. .
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2012, 21 (05) :363-369
[2]   Fracture Rates and Lifetime Estimations of CAD/CAM All-ceramic Restorations [J].
Belli, R. ;
Petschelt, A. ;
Hofner, B. ;
Hajto, J. ;
Scherrer, S. S. ;
Lohbauer, U. .
JOURNAL OF DENTAL RESEARCH, 2016, 95 (01) :67-73
[3]   Fatigue and damage accumulation of veneer porcelain pressed on Y-TZP [J].
Bonfante, Estevam A. ;
Coelho, Paulo G. ;
Guess, Petra C. ;
Thompson, Van P. ;
Silva, Nelson R. F. A. .
JOURNAL OF DENTISTRY, 2010, 38 (04) :318-324
[4]   Influence of hydrothermal and mechanical conditions on the strength of zirconia [J].
Borchers, Lothar ;
Stiesch, Meike ;
Bach, Friedrich-Wilhelm ;
Buhl, Josef-Christian ;
Huebsch, Christoph ;
Kellner, Tim ;
Kohorst, Philipp ;
Jendras, Michael .
ACTA BIOMATERIALIA, 2010, 6 (12) :4547-4552
[5]   Surface crystalline phases and nanoindentation hardness of explanted zirconia femoral heads [J].
Catledge, SA ;
Cook, M ;
Vohra, YK ;
Santos, EM ;
McClenny, MD ;
Moore, KD .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2003, 14 (10) :863-867
[6]  
Cattani-Lorente M., 2016, DENT MAT
[7]   What future for zirconia as a biomaterial? [J].
Chevalier, J .
BIOMATERIALS, 2006, 27 (04) :535-543
[8]  
Chevalier J, 1999, J AM CERAM SOC, V82, P2150
[9]   Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis [J].
Chevalier, J ;
Deville, S ;
Münch, E ;
Jullian, R ;
Lair, F .
BIOMATERIALS, 2004, 25 (24) :5539-5545
[10]   Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia [J].
Deville, S ;
Chevalier, J ;
Gremillard, L .
BIOMATERIALS, 2006, 27 (10) :2186-2192