Microstructure, magnetic and mechanical properties of Fe-28Cr-15Co-1Si cast magnets containing Mo and Ti additives

被引:4
|
作者
Zonoozi, Elnaz Mohseni [1 ]
Kianvash, Abbas [1 ]
机构
[1] Univ Tabriz, Inst Mech Engn, Dept Mat Engn, Tabriz 1476651666, Iran
来源
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING | 2020年 / 126卷 / 09期
关键词
Fe-Cr-Co-based cast permanent magnets; Spinodal decomposition; Magnetic properties; Internal stresses; Hardness; CR-CO ALLOY; HIGH-STRENGTH; EVOLUTION; PHASE; TEXTURE;
D O I
10.1007/s00339-020-03897-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the development of Fe-28Cr-15Co-1Si-xM, M = Ti and Mo,x = 1, 2, 3 (wt.%) cast permanent magnets by a thermomagnetic treatment was investigated. The alloys were melted in a vacuum induction furnace (VIM) using pure raw materials and then cast in alumina tubes. Structural, mechanical, and magnetic properties of the alloys were evaluated at different stages of heat treatment. Specimens in the solution annealed condition, showed a coarse grain with a body-centered cubic (BCC) structure (alpha phase), which decomposes into two alpha(1)and alpha(2)phases by a spinodal transformation during the thermomagnetic treatment. By addition of Mo to Fe-28Cr-15Co-1Si alloy, the strain energy of decomposition increases by concentrating in the alpha(2)phase. This results in a difference in the lattice parameter between alpha(1)and alpha(2)phases and an improvement in the magnetic properties of the alloy. The presence of Ti in the alloys raised the amount of alpha(1)phase, which eventuates in the suppression of the unwanted sigma or gamma phases in the annealed state. Ti and Mo additions also affect the development of shape anisotropy in the ferromagnetic alpha(1)particles, which in turn improves the magnetic properties of the alloys. The best magnetic properties turn out to be in Fe-28Cr-15Co-1Si-3Mo, and Fe-28Cr-15Co-1Si-2 Ti alloys:B-r = 0.98 T (9.8 kg),H-c = 67.66 kA/m (0.85 kOe) and (BH)(max) = 41.27 kJ/m(3)(5.2 MGOe), andB(r) = 0.93 T (9.3 kg),H-c = 65.27 kA/m (0.82 kOe) and (BH)(max) = 38.09 kJ/m(3)(4.8 MGOe), respectively. The hardness test results verified that in the Fe-Cr-Co-based alloys with spinodally decomposed structure, the internal stresses are more effectual than composition gradients on the alloy's strength.
引用
收藏
页数:9
相关论文
共 50 条
  • [21] Effect of Al Content on Microstructure, Mechanical, and Corrosion Properties of (Fe33Cr36Ni15Co15Ti1)100-xAlx High-Entropy Alloys
    Zheng, Qifeng
    Lu, Weiyan
    Han, Dong
    Li, Tianrun
    Guo, Hui
    Qiu, Keqiang
    Yang, Baijun
    Wang, Jianqiang
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (22)
  • [22] Microstructure, Mechanical and Corrosion Properties of Friction StirWelding High Nitrogen Martensitic Stainless Steel 30Cr15Mo1N
    Geng, Xin
    Feng, Hao
    Jiang, Zhouhua
    Li, Huabing
    Zhang, Binbin
    Zhang, Shucai
    Wang, Qi
    Li, Jizhong
    METALS, 2016, 6 (12)
  • [23] Anisotropy in microstructure and tensile properties of Ti-5Al-5Mo-5V-1Cr-1Fe produced via additive manufacturing
    Liu, Zheng
    Zhao, ZiBo
    Liu, Jianrong
    Wang, Qingjiang
    Guo, Zhenghua
    Wang, Jie
    Yang, Guang
    Gong, Shuili
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 798
  • [24] Influence of Austenitizing Temperature on the Microstructure and Mechanical Properties of an Fe-Cr-Ni-Mo-Ti Maraging Stainless Steel
    Lian, Yong
    Ma, Minyu
    Zhang, Jin
    Huang, Jinfeng
    Gao, Wen
    Zhang, Zunjun
    Zhao, Chao
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (09) : 5466 - 5475
  • [25] Effect of Co, Ti and Cr Additions on Microstructure, Magnetic Properties and Corrosion Resistance of Magnetocaloric Gd-Ge-Si Alloys
    Hasiak, Mariusz
    Checmanowski, Jacek G.
    Kucharska, Barbara
    Laszcz, Amadeusz
    Kolano-Burian, Aleksandra
    Kaleta, Jerzy
    MATERIALS, 2020, 13 (24) : 1 - 11
  • [26] The effect of ageing on microstructure and mechanical properties of powder Ti-5Al-5Mo-5V-1Cr-1Fe alloy
    Ahmed, Mansur
    Savvakin, Dmytro G.
    Ivasishin, Orest M.
    Pereloma, Elena V.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 605 : 89 - 97
  • [27] Synergistic effect of Ti, B, Si, and C on microstructure and mechanical properties of as-cast Al0.4Co0.9Cr1.2Fe0.9Ni1.2(Si, Ti, C, B)0.375 complex concentrated alloy
    Lapin, Juraj
    Klimova, Alena
    Pelachova, Tatiana
    Stamborska, Michaela
    Bajana, Oto
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 934
  • [28] Microstructure and mechanical properties of Co-28Cr-6Mo-0.22C investment castings by current solution treatment
    Dan, Ze-yu
    Liu, Jun
    Zhang, Jian-lei
    Li, Yan-hua
    Deng, Yuan-xin
    Zhang, Yun-hu
    Song, Chang-jiang
    CHINA FOUNDRY, 2024, 21 (04) : 369 - 378
  • [29] Mechanical properties and microstructure in a fine grained Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy deformed at a high strain rate
    Wang, Bingfeng
    Yao, XianRui
    Liu, Lanyi
    Zhang, Xiaoyong
    Ding, Xu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 736 : 202 - 208
  • [30] Effect of Annealing Process on Microstructure, Texture, and Mechanical Properties of a Fe-Si-Cr-Mo-C Deep Drawing Dual-Phase Steel
    Pan, Hongbo
    Shen, Xiaohui
    Li, Dongyang
    Liu, Yonggang
    Cao, Jinghua
    Tian, Yaqiang
    Zhan, Hua
    Wang, Huiting
    Wang, Zhigang
    Xiao, Yangyang
    CRYSTALS, 2020, 10 (09): : 1 - 16