L-Ascorbic Acid as an Efficient Green Corrosion Inhibitor of Steel Rebars in Chloride Contaminated Cement Mortar

被引:8
作者
Argiz, Cristina [1 ]
Arroyo, Celia [1 ]
Bravo, Astrid [1 ]
Moragues, Amparo [1 ]
Andrade, Carmen [2 ]
Bolzoni, Fabio [3 ]
机构
[1] Univ Politecn Madrid, ETSI Caminos Canales & Puertos, Madrid 20040, Spain
[2] Ctr Int Metodos Numer Ingn CIMNE, Madrid 08034, Spain
[3] Politecn Milan, I-20133 Milan, Italy
关键词
green corrosion inhibitor; ascorbic acid; chloride-contaminated mortars; linear polarization resistance; electrochemical impedance spectroscopy; differential thermal; thermogravimetric analysis; VITAMIN-C; REINFORCED-CONCRETE; PORTLAND-CEMENT; CARBON-STEEL; DEGRADATION; HYDRATION; POLARIZATION; CHEMISTRY; MECHANISM; PHOSPHATE;
D O I
10.3390/ma15228005
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Corrosion of reinforcement is a major problem regarding concrete durability. In new structures the corrosion onset can be delayed if additional protection methods are provided as is the case for the addition of corrosion inhibitors in the concrete mix. The main goal of this paper is the evaluation of the effect of the ascorbic acid (AA) as a green steel corrosion inhibitor in cement mortars contaminated by chlorides. Concentration levels of ascorbic acid, ranging from 0.5 to 10(-3) mol/L, were added to the mixing water. Electrochemical methods, including corrosion potential (Ecorr), linear polarization resistance (LPR) and electrochemical impedance spectroscopy (EIS), were employed to assess the corrosion rate of the steel embedded in the mortars. The corrosion inhibiting performance of ascorbic acid was compared with that of sodium nitrite. The interaction of the ascorbic acid with the hydrated cement matrix was also evaluated with differential thermal and thermogravimetric analysis (DTA/TG) and pH measurements. The results indicated that, depending on the ascorbic acid concentration, it can be an activator of the corrosion process or an effective corrosion inhibitor in a similar manner to sodium nitrite. A corrosion rate decrease was achieved with concentrations below 10(-2) mol/L and the optimum content was 10(-3) mol/L. Within this concentration range, the AA does not modify the hydration performance of the cement matrix.
引用
收藏
页数:19
相关论文
共 62 条
  • [1] Effect of non-toxic corrosion inhibitors on steel in chloride solution
    Akrout, H
    Bousselmi, L
    Triki, E
    Maximovitch, S
    Dalard, F
    [J]. JOURNAL OF MATERIALS SCIENCE, 2004, 39 (24) : 7341 - 7350
  • [2] Chloride threshold values to depassivate reinforcing bars embedded in a standardized OPC mortar
    Alonso, C
    Andrade, C
    Castellote, M
    Castro, P
    [J]. CEMENT AND CONCRETE RESEARCH, 2000, 30 (07) : 1047 - 1055
  • [3] Alonso M., 2011, P 13 INT C CHEM CEME
  • [4] Test methods for on-site corrosion rate measurement of steel reinforcement in concrete by means of the polarization resistance method
    Andrade, C
    Alonso, C
    Gulikers, J
    Polder, R
    Cigna, R
    Vennesland, O
    Salta, M
    Raharinaivo, A
    Elsener, B
    [J]. MATERIALS AND STRUCTURES, 2004, 37 (273) : 623 - 643
  • [5] QUANTITATIVE MEASUREMENTS OF CORROSION RATE OF REINFORCING STEELS EMBEDDED IN CONCRETE USING POLARIZATION RESISTANCE MEASUREMENTS
    ANDRADE, C
    GONZALEZ, JA
    [J]. WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1978, 29 (08): : 515 - 519
  • [6] Anejjar A., 2017, Appl. J. Envir. Eng. Sci., V3, P36, DOI [10.48422/IMIST.PRSM/ajees-v3i1.7432, DOI 10.48422/IMIST.PRSM/AJEES-V3I1.7432, 10.48422/IMIST.PRSM/AJEES-V3I1.7432]
  • [7] Critical chloride content in reinforced concrete - A review
    Angst, Ueli
    Elsener, Bernhard
    Larsen, Claus K.
    Vennesland, Oystein
    [J]. CEMENT AND CONCRETE RESEARCH, 2009, 39 (12) : 1122 - 1138
  • [8] Effect of calcium nitrite-based corrosion inhibitor in preventing corrosion of embedded steel in concrete
    Ann, KY
    Jung, HS
    Kim, HS
    Kim, SS
    Moon, HY
    [J]. CEMENT AND CONCRETE RESEARCH, 2006, 36 (03) : 530 - 535
  • [9] [Anonymous], 2019, D497213 ASTM INT
  • [10] [Anonymous], 2016, C87615 ASTM INT