TWIP Effect and Plastic Instability Condition in an Fe-Mn-C Austenitic Steel

被引:68
|
作者
Koyama, Motomichi [1 ]
Sawaguchi, Takahiro [1 ]
Tsuzaki, Kaneaki [1 ,2 ]
机构
[1] Natl Inst Mat Sci, Tsukuba, Ibaraki 3050047, Japan
[2] Univ Tsukuba, Tsukuba, Ibaraki 3050047, Japan
基金
日本学术振兴会;
关键词
high carbon; high Mn steel; austenitic steel; twinning-induced plasticity; work hardening; dynamic strain aging; EPSILON-MARTENSITIC-TRANSFORMATION; HADFIELD MANGANESE STEEL; STACKING-FAULT ENERGY; MECHANICAL-PROPERTIES; TENSILE BEHAVIOR; DEFORMATION; DISLOCATION; BOUNDARIES; GRAIN; FRACTURE;
D O I
10.2355/isijinternational.53.323
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
We investigated the correlation among deformation twin density, work hardening, and tensile ductility in an Fe-18Mn-1.2C twinning-induced-plasticity (TWIP) steel, and discussed the correlation with the plastic instability condition. The deformation twin density was varied by changing the deformation temperature from 123 to 523 K. An important factor for the uniform elongation is the work hardening rate in a later deformation stage. The increase in the deformation twin density enhanced the work hardening rate significantly but not monotonically just before the fracture, since the deformation twin density is saturated against plastic strain. In addition, dynamic strain aging in a later deformation stage and epsilon-martensitic transformation were found to accelerate the fracture due to the localized deformation and the premature fracture, respectively. Accordingly, the relationship between uniform elongation and deformation twin density was not simple. The optimum conditions for the TWIP effect were concluded to be (1) considerable amount of deformation twinning in a later deformation stage, (2) suppression of dynamic strain aging in a later deformation stage, and (3) inhibition of epsilon-martensitic transformation.
引用
收藏
页码:323 / 329
页数:7
相关论文
共 50 条
  • [1] TWIP Effect and Plastic Instability Condition in an Fe-Mn-C Austenitic Steel
    Koyama, Motomichi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2012, 98 (06): : 229 - 236
  • [2] Effect of deformation temperature on tensile properties in a pre-cooled Fe-Mn-C austenitic steel
    Koyama, Motomichi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 331 - 336
  • [3] Room-temperature blue brittleness of Fe-Mn-C austenitic steels
    Koyama, Motomichi
    Shimomura, Yusaku
    Chiba, Aya
    Akiyama, Eiji
    Tsuzaki, Kaneaki
    SCRIPTA MATERIALIA, 2017, 141 : 20 - 23
  • [4] Influence of Dislocation Separation on Dynamic Strain Aging in a Fe-Mn-C Austenitic Steel
    Koyama, Motomichi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    MATERIALS TRANSACTIONS, 2012, 53 (03) : 546 - 552
  • [5] Overview of Dynamic Strain Aging and Associated Phenomena in Fe-Mn-C Austenitic Steels
    Koyama, Motonnchi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2018, 104 (04): : 187 - 200
  • [6] Overview of Dynamic Strain Aging and Associated Phenomena in Fe-Mn-C Austenitic Steels
    Koyama, Motomichi
    Sawaguchi, Takahiro
    Tsuzaki, Kaneaki
    ISIJ INTERNATIONAL, 2018, 58 (08) : 1383 - 1395
  • [7] Twinning and dynamic strain aging behavior during tensile deformation of Fe-Mn-C TWIP steel
    Lan, Peng
    Zhang, Jiaquan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 700 : 250 - 258
  • [8] Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe-Mn-C TWIP steels
    Dieudonne, T.
    Marchetti, L.
    Wery, M.
    Chene, J.
    Allely, C.
    Cugy, P.
    Scott, C. P.
    CORROSION SCIENCE, 2014, 82 : 218 - 226
  • [9] Serrated Flow and Dynamic Strain Aging in Fe-Mn-C TWIP Steel
    Lan, Peng
    Zhang, Jiaquan
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (01): : 147 - 161
  • [10] Hydrogen-induced cracking at grain and twin boundaries in an Fe-Mn-C austenitic steel
    Koyama, Motomichi
    Akiyama, Eiji
    Sawaguchi, Takahiro
    Raabe, Dierk
    Tsuzaki, Kaneaki
    SCRIPTA MATERIALIA, 2012, 66 (07) : 459 - 462