共 55 条
Porous-crystalline C/Fe3O4 microspheres with highly accessible adsorptive/catalytic and conductive interfaces to manipulate polysulfide shuttling in Li-S batteries
被引:11
作者:
Adi, Akylbek
[1
]
Taniguchi, Izumi
[1
]
机构:
[1] Tokyo Inst Technol, Dept Chem Sci & Engn, Tokyo 1528552, Japan
关键词:
Spray pyrolysis;
Steam oxidation;
Porous-crystalline C/Fe3O4 microspheres;
Polysulfide adsorption;
Li-S batteries;
LITHIUM-SULFUR BATTERIES;
ELECTROCHEMICAL PROPERTIES;
SPRAY-PYROLYSIS;
PERFORMANCE;
SEPARATOR;
CHEMISTRY;
FRAMEWORK;
D O I:
10.1016/j.electacta.2022.141385
中图分类号:
O646 [电化学、电解、磁化学];
学科分类号:
081704 ;
摘要:
We used different C/Fe3O4 microspheres such as dense-amorphous and porous-crystalline, prepared by spray pyrolysis with steam oxidation, to clarify the synergetic effect of conductive and adsorptive/catalytic interfaces on the electrochemical properties of Li-S batteries. According to the physical characterizations, the prepared C/Fe3O4 microspheres significantly differ in their surface texture, porosity, and crystal structures. The porouscrystalline C/Fe3O4 microspheres have a wide range of micro-and mesopores to physically adsorb polysulfides and highly accessible Fe3O4 nanoparticles to chemically immobilize them within the electrochemical interfaces and promote their conversion into short-chain sulfides. On the other hand, a densely coated carbon of the denseamorphous C/Fe3O4 microspheres impedes the chemical interaction between the polysulfides and Fe3O4 nanoparticles. As a result, the porous-crystalline C/Fe3O4 microspheres enhance sulfur utilization and accelerate the redox kinetics of Li-S cells when used as modified separators. These cells exhibit a higher specific capacity of similar to 700 mAh g(-1) with a capacity retention of 93% after 200 cycles at 1.0 C. This work demonstrates that high-performance Li-S batteries can be achieved by rationally designing conductive and adsorptive/catalytic interfaces of C/Fe3O4 microspheres.