共 22 条
Preparation and Properties of Stable Suspensions of ZrO2-Y2O3 Powders with Different Particle Sizes for Electrophoretic Deposition
被引:5
作者:
Kalinina, E. G.
[1
,2
]
Pikalova, E. Yu.
[2
,3
]
机构:
[1] Russian Acad Sci, Inst Electrophys, Ural Branch, Ekaterinburg 620016, Russia
[2] Ural Fed Univ, Ekaterinburg 620002, Russia
[3] Russian Acad Sci, Inst High Temperature Electrochem, Ural Branch, Ekaterinburg 620137, Russia
关键词:
electrophoretic deposition;
stable suspension;
aggregates;
YSZ;
thin film;
ELECTROLYTE THIN-FILMS;
ZIRCONIA;
EVAPORATION;
YSZ;
D O I:
10.1134/S0020168520090095
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
This paper presents a study of nonaqueous suspensions based on ZrO2-8 mol % Y2O3(8YSZ) powders and describes the use of the powders for producing thin-film coatings on a La2NiO4(LNO) substrate by electrophoretic deposition (EPD). Stable suspensions for EPD have been prepared using 8YSZ powders differing in morphology and particle size: nanopowder (YSZ_L) produced by a laser evaporation-condensation process and commercially available powder (YSZ_T) (Tosoh, Japan). Ultrasonic processing has been found to have different effects on the particle size composition of the YSZ_L and YSZ_T suspensions. The two types of suspension have been shown to differ significantly in the kinetics of the deposition current at constant voltage: during deposition from the YSZ_L suspension, the current was observed to rise, whereas in the case of the YSZ_T suspension the current decreased markedly with deposition time. The YSZ_L film has been shown to be denser than the YSZ_T film. After sintering at 1350 degrees C, it consisted of completely formed grains ranging in size from 1 to 5 mu m. To remove surface pores in YSZ_T coatings, they should be sintered at a temperature of 1450 degrees C.
引用
收藏
页码:941 / 948
页数:8
相关论文