Effects of Solution-Annealing Temperature on the Precipitation of Secondary Phases and the Associated Pitting Corrosion Resistance in Hyper Duplex Stainless Steel

被引:17
作者
Jeon, Soon-Hyeok [1 ]
Kim, Soon-Tae [1 ]
Kim, Se-Young [1 ]
Choi, Min-Seok [1 ]
Park, Yong-Soo [1 ]
机构
[1] Yonsei Univ, Dept Mat Sci & Engn, Seoul 120749, South Korea
关键词
duplex stainless steel; pitting corrosion; solution heat treatment; secondary phase; SIGMA-PHASE; MECHANICAL-PROPERTIES; MICROSTRUCTURAL STABILITY; CHLORIDE SOLUTIONS; INCLUSIONS; NITROGEN;
D O I
10.2320/matertrans.M2012402
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of the solution-annealing temperature on the precipitation of secondary phases and the associated pitting corrosion resistance in hyper duplex stainless steel after aging at 1123K were investigated in a highly concentrated chloride solution. Increasing the solution annealing temperature from 1333 to 1413 K retarded the formation of the secondary phases owing to a decrease in both the number of preferential precipitation sites such as the ferrite/austenite interface and the activities of Cr, Mo and W. The slow rate of degradation of the pitting corrosion resistance of the alloy with the increase in the solution annealing temperature appears to be caused by the retardation of the precipitation of the sigma phase. Based on the results of the precipitation of secondary phases and electrochemical tests, the optimal solution annealing temperature was determined to be 1373 K.
引用
收藏
页码:1473 / 1479
页数:7
相关论文
共 32 条
[1]   THERMO-CALC & DICTRA, computational tools for materials science [J].
Andersson, JO ;
Helander, T ;
Höglund, LH ;
Shi, PF ;
Sundman, B .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2002, 26 (02) :273-312
[2]  
[Anonymous], ANN BOOK ASTM STAND
[3]  
Bernhardsson S., 1991, Duplex Stainless Steels '91, V1, P185
[4]   The effect of high-temperature exposure on the microstructural stability and toughness property in a 2205 duplex stainless steel [J].
Chen, TH ;
Weng, KL ;
Yang, JR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 338 (1-2) :259-270
[5]   Effects of solution treatment and continuous cooling on σ-phase precipitation in a 2205 duplex stainless steel [J].
Chen, TH ;
Yang, JR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 311 (1-2) :28-41
[6]   Effect of thermal cycles on the corrosion and mechanical properties of UNS S31803 duplex stainless steel [J].
Deng, Bo ;
Wang, Zhiyu ;
Jiang, Yiming ;
Sun, Tao ;
Xu, Juliang ;
Li, Jin .
CORROSION SCIENCE, 2009, 51 (12) :2969-2975
[7]   Energy-dispersive spectroscopy and electron backscatter diffraction analysis of isothermally aged SAF 2507 type superduplex stainless steel [J].
Dobranszky, J ;
Szabo, PJ ;
Berecz, T ;
Hrotko, V ;
Portko, M .
SPECTROCHIMICA ACTA PART B-ATOMIC SPECTROSCOPY, 2004, 59 (10-11) :1781-1788
[8]   The effect of phase compositions on the pitting corrosion of 25 Cr duplex stainless steel in chloride solutions [J].
GarfiasMesias, LF ;
Sykes, JM ;
Tuck, CDS .
CORROSION SCIENCE, 1996, 38 (08) :1319-1330
[9]  
Hertzman S, 1995, SCAND J METALL, V24, P140
[10]   Effects of nitrogen and high temperature aging on σ phase precipitation of duplex stainless steel [J].
Huang, CS ;
Shih, CC .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 402 (1-2) :66-75