Interpenetration, Porosity, and High-Pressure Gas Adsorption in Zn4O(2,6-naphthalene dicarboxylate)3

被引:33
作者
Feldblyum, Jeremy I. [1 ,2 ]
Dutta, Dhanadeep [3 ]
Wong-Foy, Antek G. [2 ]
Dailly, Anne [4 ]
Imirzian, James [3 ]
Gidley, David W. [3 ]
Matzger, Adam J. [1 ,2 ]
机构
[1] Univ Michigan, Ann Arbor, MI 48109 USA
[2] Univ Michigan, Dept Chem, Ann Arbor, MI 48109 USA
[3] Univ Michigan, Dept Phys, Ann Arbor, MI 48109 USA
[4] Gen Motors Global R&D, Warren, MI 48090 USA
基金
美国国家科学基金会;
关键词
METAL-ORGANIC FRAMEWORKS; PORE-SIZE DISTRIBUTIONS; HYDROGEN STORAGE; COORDINATION POLYMERS; POSITRON-ANNIHILATION; SURFACE-AREAS; DESIGN; SATURATION; SORPTION; CONSTRUCTION;
D O I
10.1021/la401323t
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Microporous coordination polymers (MCPs) have emerged as strong contenders for adsorption-based fuel storage and delivery in large part because of their high specific surface areas. The strategy of increasing surface area by increasing organic linker length has shown only sporadic success; as demonstrated by many members of the iconic Zn4O-based IRMOF series, for example, accessible porosity is often limited by interpenetration or pore collapse upon guest removal. In this work, we focus on Zn4O(ndc)(3) (IRMOF-8, ndc = 2,6-naphthalene dicarboxylate), which exhibits typical surface areas of only 1000-2000 m(2)/g even though a surface area of more than 4000 m(2)/g is expected from geometric analysis of the originally reported crystal structure. We recently showed that a high surface area could be produced with zinc and ndc by room-temperature synthesis followed by activation with flowing supercritical CO2. In this work, we investigate in detail the porosity of both the low- and high-surface-area materials. Positron annihilation lifetime spectroscopy (PALS) is used to show that the low-surface-area material suffers from near-complete interpenetration, explaining why traditional synthetic routes have failed to yield materials with the expected porosity. Furthermore, the high-pressure hydrogen and methane sorption properties of noninterpenetrated Zn4O(ndc)(3) are examined, and PALS is used to show that pore filling is not operative during room-temperature CH4 sorption even at pressures approaching 100 bar. These results provide insight into how gas adsorbs in high-surface-area materials at high pressure and reinforce previous contentions that increasing surface area alone is not sufficient for the simultaneous optimization of deliverable gravimetric and volumetric gas uptake in MCPs.
引用
收藏
页码:8146 / 8153
页数:8
相关论文
共 60 条
[1]   ASSEMBLY OF PORPHYRIN BUILDING-BLOCKS INTO NETWORK STRUCTURES WITH LARGE CHANNELS [J].
ABRAHAMS, BF ;
HOSKINS, BF ;
MICHAIL, DM ;
ROBSON, R .
NATURE, 1994, 369 (6483) :727-729
[2]  
[Anonymous], TARG ONB HYDR STOR S
[3]   On the enhancement of hydrogen uptake by IRMOF-8 composites with Pt/carbon catalyst [J].
Ardelean, Ovidiu ;
Blanita, Gabriela ;
Borodi, Gheorghe ;
Mihet, Maria ;
Coros, Maria ;
Lupu, Dan .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2012, 37 (09) :7378-7384
[4]   Optimal isosteric heat of adsorption for hydrogen storage and delivery using metal-organic frameworks [J].
Bae, Youn-Sang ;
Snurr, Randall Q. .
MICROPOROUS AND MESOPOROUS MATERIALS, 2010, 132 (1-2) :300-303
[5]   Strategies for Characterization of Large-Pore Metal-Organic Frameworks by Combined Experimental and Computational Methods [J].
Bae, Youn-Sang ;
Dubbeldam, David ;
Nelson, Andrew ;
Walton, Krista S. ;
Hupp, Joseph T. ;
Snurr, Randall Q. .
CHEMISTRY OF MATERIALS, 2009, 21 (20) :4768-4777
[6]  
Batten SR, 1998, ANGEW CHEM INT EDIT, V37, P1460, DOI 10.1002/(SICI)1521-3773(19980619)37:11<1460::AID-ANIE1460>3.0.CO
[7]  
2-Z
[8]   Optimum conditions for adsorptive storage [J].
Bhatia, SK ;
Myers, AL .
LANGMUIR, 2006, 22 (04) :1688-1700
[9]   Fast method for computing pore size distributions of model materials [J].
Bhattacharya, Supriyo ;
Gubbins, Keith E. .
LANGMUIR, 2006, 22 (18) :7726-7731
[10]  
Caskey SR., 2009, Mater Matters, V4, P111