Properties of a thermoplastic composite skin-stiffener interface in a stiffened structure manufactured by laser-assisted tape placement with in situ consolidation

被引:29
作者
Bandaru, Aswani Kumar [1 ]
Clancy, Gearoid [1 ]
Peeters, Daniel [1 ,2 ]
O'Higgins, Ronan M. [1 ]
Weaver, Paul M. [1 ]
机构
[1] Univ Limerick, Sch Engn, Bernal Inst, Irish Ctr Composites Res IComp, Limerick, Ireland
[2] Delft Univ Technol, Fac Aerosp Engn, Kluyverweg 1, NL-2629 HS Delft, Netherlands
基金
欧盟地平线“2020”; 爱尔兰科学基金会;
关键词
Automated fibre placement; Thermoplastic; Mechanical testing; Interface properties; INTERLAMINAR FRACTURE-TOUGHNESS; CARBON FIBRE/PEEK COMPOSITES; COOLING RATE INFLUENCES; DELAMINATION; PARAMETERS; STRENGTH;
D O I
10.1016/j.compstruct.2019.02.011
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
A critically important consideration of stiffened structural panels is the interfacial properties between skin and stiffener. In the present study a novel implementation of laser-assisted tape placement (LATP) was used to produce a representative skin-stiffener of a wingbox from carbon fibre reinforced PEEK. First, a stiffener is manufactured using this method and subsequently the skin is attached using the same method without need for a secondary bonding process. The interfacial properties between the skin and stiffener have been characterised in terms of interlaminar shear strength (ILSS) and fracture toughness (Mode-I and Mode-II) properties. LATP laydown direction and laser power was found to influence the skin-stiffener interface Mode-I fracture toughness, but not affect the Mode-II fracture toughness. The values of ILSS and fracture toughness compare favourably with those results reported in the literature, in particular for those reported for equivalent aerospace certified CF/PEEK material (APC-2).
引用
收藏
页码:123 / 131
页数:9
相关论文
共 27 条
  • [1] The thermoplastic laser-assisted consolidation process-mechanical and microstructure characterization
    Agarwal, V
    McCullough, RL
    Schultz, JM
    [J]. JOURNAL OF THERMOPLASTIC COMPOSITE MATERIALS, 1996, 9 (04) : 365 - 380
  • [2] [Anonymous], 2016, D2344 ASTM
  • [3] [Anonymous], 2014, D7905 ASTM
  • [4] [Anonymous], 2013, D5528 ASTM
  • [5] Effect of fibre content on the interlaminar fracture toughness of unidirectional glass-fibre/polyamide composite
    Chen, JH
    Schulz, E
    Bohse, J
    Hinrichsen, G
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (06) : 747 - 755
  • [6] Mechanical characterisation of carbon fibre-PEEK manufactured by laser-assisted automated-tape-placement and autoclave
    Comer, A. J.
    Ray, D.
    Obande, W. O.
    Jones, D.
    Lyons, J.
    Rosca, I.
    O'Higgins, R. M.
    McCarthy, M. A.
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 69 : 10 - 20
  • [7] Influence of ENF specimen geometry and friction on the mode II delamination resistance of carbon/PEEK
    Davies, P
    [J]. JOURNAL OF THERMOPLASTIC COMPOSITE MATERIALS, 1997, 10 (04) : 353 - 361
  • [8] Automated manufacturing and processing of fiber-reinforced polymer (FRP) composites: An additive review of contemporary and modern techniques for advanced materials manufacturing
    Frketic, Jolie
    Dickens, Tarik
    Ramakrishnan, Subramanian
    [J]. ADDITIVE MANUFACTURING, 2017, 14 : 69 - 86
  • [9] Cooling rate influences in carbon fibre/PEEK composites. Part II: interlaminar fracture toughness
    Gao, SL
    Kim, JK
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2001, 32 (06) : 763 - 774
  • [10] Cooling rate influences in carbon fibre/PEEK composites. Part 1. Crystallinity and interface adhesion
    Gao, SL
    Kim, JK
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2000, 31 (06) : 517 - 530